MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zoltek™ PX30 Carbon Fiber Roving
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK PX30 High-Twist Roving is manufactured with high twist to improve its handling characteristics. The roving is widely used as a baseline material for the manufacture of friction clutches and brakes. Thick fabrics woven of ZOLTEK PX30 High-Twist Roving allow for efficient buildup during fabrication of composite substructures.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 99 %99 %
 
Descriptive Properties
Denier4465g
Oxidation Rate1.0% per hour @ 932°F
Turns per Inch1.7
Twisting DirectionS or Z
Yield (m/kg)2015

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ PX35 Milled Carbon Fiber
Zoltek™ PX30 SW08 (Satin Weave) Carbon Fiber Fabric
Zoltek™ PX30YS0205 Carbon Fiber Yarn
Zoltek™ PX30YS0505 Carbon Fiber Yarn
Carlisle 201LL Carbon-Carbon Composite

ECZO828 / 232300

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.