MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Capron® 8351 Impact Modified Nylon 6 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also available in heat stabilized (Capron 8351 HS) and/or pigmented versions.

Capron 8351 is generally recommended for applications such as storage bins, spray gun and power tool handles, trim clips and fasteners, wall anchors, and automotive roof racks.

Data provided by Allied Signal.

Processing: Max. water content 0.2%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 240-270 degC (464-518 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of 10-95 degC (50-203 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO data
Water Absorption 1.1 %1.1 %24 hrs; ISO data
Moisture Absorption at Equilibrium 1.9 %1.9 %50% RH; 23°C; ISO data
Water Absorption at Saturation 6.7 %6.7 %in water; 23°C; ISO data
Linear Mold Shrinkage 0.013 cm/cm0.013 in/inISO data
 0.014 cm/cm0.014 in/inASTM data MD
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inISO Data
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7979ASTM Data
Tensile Strength, Yield 50.0 MPa7250 psiASTM value at 50 mm/min.
 52.0 MPa7540 psiISO value at 50 mm/min.
Elongation at Break >= 50 %>= 50 %Nominal
 >= 100 %>= 100 %Nominal
Elongation at Yield 7.0 %7.0 %ISO Value at 50 mm/min.
 7.0 %7.0 %ASTM Value at 50 mm/min.
Flexural Yield Strength 65.0 MPa9430 psiASTM Data
Flexural Modulus 1.40 GPa203 ksiISO Value
 1.655 GPa240.0 ksiASTM Value
Poissons Ratio 0.350.35ISO data
Charpy Impact, Notched NBNBISO Data
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmISO data
Dielectric Strength 20.0 kV/mm508 kV/inISO data
Comparative Tracking Index 600 V600 VISO data
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 20.0 °C
11.1 µin/in-°F
@Temperature 68.0 °F
ISO data
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 20.0 °C
61.1 µin/in-°F
@Temperature 68.0 °F
ISO data
Melting Point 220 °C428 °FASTM and ISO test
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °FISO data
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C118 °FISO data
 53.0 °C127 °FASTM Data
Flammability, UL94  HB
@Thickness 0.810 mm
HB
@Thickness 0.0319 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 280 °C536 °FSee Materials Notes
Mold Temperature 70.0 °C158 °FSee Materials Notes
Drying Temperature 85.0 °C185 °FSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8253 PA6 (Dry)
BASF Capron® 1943 Impact Modified Nylon 6 (Dry)
Overview of materials for Nylon 6, Impact Grade
BASF Ultramid® 8253 PA6 (Conditioned)
Celanese Zytel® ST811HS NC010 PA6-HI

PALD13 / 23907

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.