MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Precite® P3 ICF 20 black (6947) Polybutylene Terephthalate (PBT), Carbon Fiber
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Carbon Fiber Filled

Material Notes: Carbon Fiber Reinforced Compounds. Good surface and strength. PBT CF 20.

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183
Filler Content 20 %20 %ISO 1172
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm0.0080 - 0.010 in/inISO 294-4
Melt Flow 23.29 g/10 min
@Load 2.16 kg,
Temperature 250 °C
23.29 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 150 MPa21800 psi5 mm/min. Dry as Molded; ISO 527-2
Elongation at Break 3.0 %3.0 %5 mm/min. Dry as Molded; ISO 527-2
Tensile Modulus 16.0 GPa2320 ksi1 mm/min. Dry as Molded.; ISO 527-2
Flexural Strength 250 MPa36300 psiDry as Molded. 2 mm/min; ISO 178
Flexural Modulus 15.0 GPa2180 ksi2 mm/min. Dry as Molded; ISO 178
Charpy Impact Unnotched 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
Charpy Impact, Notched 0.750 J/cm²
@Temperature 23.0 °C
3.57 ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1000 ohm1000 ohmDry as Molded; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FDry as Molded. DES, 10°C/min; DIN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FDry as Molded; ISO 75
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Dry as Molded
Glow Wire Flammability Index 725 °C1340 °FDry as Molded; IEC 60695-2-12
 
Descriptive Properties
Burning Rate<100 mm/minDry as Molded. FMVSS 302. >1 mm thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKRO9878 / 255535

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.