HG565FB is a polypropylene homopolymer mainly intended for BCF, CF and staple fiber. HG565FB has a gasfading free stabilization package to avoid discoloration of the fibers. Cas No. 9003-07-0 Typical characteristics: - Easy processability
- Excellent spinning performance
- Gasfading free stabilization
- Optimal product consistency
- Improved long term heat stability
Applications: - Staple fiber for nonwoven
- Continuous filaments
- Bulk Continuous Filament
Information provided by Borealis AG |