MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celanex® 7714 PBT, Mineral / Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass + Mineral Filled

Material Notes: Celanex 7714 is a 35% glass/mineral reinforced, non-exuding, flame retartant PBT which has an excellent balance of mechanical properties and processability. Celanex 7714 is well suited for electrical applications where warp resistance and/or very flat su

Information provided by Celanese Corporation.

Key Words: A 35% glass/mineral reinforced, FR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.69 g/cc0.0611 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0025 - 0.0045 cm/cm0.0025 - 0.0045 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 79.0 MPa11500 psi5mm/min; ISO 527-2/1A
Elongation at Break 1.0 %1.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 11.9 GPa1730 ksi1mm/min; ISO 527-2/1A
Flexural Strength 131 MPa19000 psiISO 178
Flexural Modulus 12.0 GPa1740 ksiISO 178
Izod Impact, Notched (ISO) 3.10 kJ/m²1.48 ft-lb/in²ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+17 ohm1.00e+17 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 184 °C363 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 213 °C415 °FISO 75-1, -2
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65

PHCS098 / 123513

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.