MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

High-Nickel Ductile Iron, corrosion resistant
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Austenite matrix structure as cast.

Ni-Resist austenitic iron, ASTM A439

Key Words: Corrosion resistant high-nickel ductile iron, ASTM A439, austenitic
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.39 g/cc0.267 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 130 - 240130 - 240
Tensile Strength 380 - 480 MPa55100 - 69600 psi
Compressive Strength 1240 - 1380 MPa180000 - 200000 psi
Charpy Impact 14.0 - 40.0 J10.3 - 29.5 ft-lbStandard Charpy
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000100 ohm-cm0.000100 ohm-cmEstimated.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.6 - 18.7 µm/m-°C
@Temperature 21.0 °C
7.00 - 10.4 µin/in-°F
@Temperature 69.8 °F
Thermal Conductivity 13.4 W/m-K93.0 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 3.0 %<= 3.0 %
Chromium, Cr 1.0 - 5.5 %1.0 - 5.5 %
Iron, Fe 61 %61 %
Manganese, Mn 0.70 - 4.5 %0.70 - 4.5 %
Molybdenum, Mo <= 1.0 %<= 1.0 %
Nickel, Ni 18 - 36 %18 - 36 %
Phosphorus, P <= 0.080 %<= 0.080 %
Silicon, Si 1.0 - 3.0 %1.0 - 3.0 %
Sulfur, S <= 0.12 %<= 0.12 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ductile Iron grade 60-40-18
Medium-Silicon Ductile Iron, heat-resistant ductile iron
Carpenter Invar 36® Alloy, Cold Drawn Bars
Overview of materials for Ductile Iron
High-Nickel Ductile Iron, heat-resistant ductile iron, 20% Ni

MAFEA6 / 10236

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.