MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Description

LP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical performance. This material has excellent processability and balanced end-use properties such as environmental stress crack resistance with superior impact.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/ccASTM D1505
ESCR 100% Igepal® 500 hour500 hourCondition A; ASTM D1693
Melt Index of Compound 11 g/10 min
@Load 2.16 kg,
Temperature 190 °C
11 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363ASTM D2240
Tensile Strength, Yield 24.8 MPa3600 psiASTM D638
Elongation at Break 800 %800 %2"/min; ASTM D638
Flexural Modulus 1.14 GPa165 ksitangent; ASTM D790
Izod Impact, Notched 4.00 J/cm7.50 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C162 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR™ TECH UHMW-PE + MoS2
American Red Maple Wood
PTS Trilac® ABS-HF5500 High Flow ABS Resin
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant
American Red Oak Wood

PASHU082 / 25046

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.