MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 20% Glass Fiber Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.64 g/cc0.0434 - 0.0592 lb/in³Average value: 1.38 g/cc Grade Count:31
Filler Content 15.0 - 23.0 %15.0 - 23.0 %Average value: 18.7 % Grade Count:13
Water Absorption 0.160 - 0.300 %0.160 - 0.300 %Average value: 0.233 % Grade Count:16
Linear Mold Shrinkage 0.00200 - 0.0100 cm/cm0.00200 - 0.0100 in/inAverage value: 0.00476 cm/cm Grade Count:30
Linear Mold Shrinkage, Transverse 0.00600 - 0.0160 cm/cm0.00600 - 0.0160 in/inAverage value: 0.00853 cm/cm Grade Count:17
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 124 - 127124 - 127Average value: 125 Grade Count:8
Tensile Strength, Ultimate 75.8 - 200 MPa11000 - 29000 psiAverage value: 125 MPa Grade Count:30
 55.0 - 105 MPa
@Temperature 60.0 - 150 °C
7980 - 15200 psi
@Temperature 140 - 302 °F
Average value: 80.1 MPa Grade Count:2
Elongation at Break 1.00 - 6.00 %1.00 - 6.00 %Average value: 2.28 % Grade Count:31
 2.00 - 12.0 %
@Temperature 60.0 - 150 °C
2.00 - 12.0 %
@Temperature 140 - 302 °F
Average value: 5.25 % Grade Count:1
Elongation at Yield 3.50 - 10.0 %
@Temperature 120 - 150 °C
3.50 - 10.0 %
@Temperature 248 - 302 °F
Average value: 6.75 % Grade Count:1
Modulus of Elasticity 4.14 - 15.4 GPa600 - 2230 ksiAverage value: 8.11 GPa Grade Count:29
 2.00 - 6.80 GPa
@Temperature 60.0 - 150 °C
290 - 986 ksi
@Temperature 140 - 302 °F
Average value: 5.12 GPa Grade Count:2
Flexural Yield Strength 110 - 226 MPa16000 - 32800 psiAverage value: 173 MPa Grade Count:24
 66.9 - 141 MPa
@Temperature 100 - 100 °C
9700 - 20500 psi
@Temperature 212 - 212 °F
Average value: 104 MPa Grade Count:2
Flexural Modulus 4.14 - 9.65 GPa600 - 1400 ksiAverage value: 6.97 GPa Grade Count:25
 2.34 - 4.96 GPa
@Temperature 100 - 100 °C
339 - 719 ksi
@Temperature 212 - 212 °F
Average value: 3.65 GPa Grade Count:2
Compressive Yield Strength 100 - 207 MPa14500 - 30000 psiAverage value: 155 MPa Grade Count:4
Poissons Ratio 0.350 - 0.4100.350 - 0.410Average value: 0.362 Grade Count:3
Shear Strength 56.5 - 88.0 MPa8190 - 12800 psiAverage value: 73.8 MPa Grade Count:4
Izod Impact, Notched 0.180 - 1.87 J/cm0.337 - 3.50 ft-lb/inAverage value: 0.545 J/cm Grade Count:21
Izod Impact, Unnotched 2.67 - 9.60 J/cm5.00 - 18.0 ft-lb/inAverage value: 4.92 J/cm Grade Count:15
Izod Impact, Notched (ISO) 2.50 - 12.0 kJ/m²1.19 - 5.71 ft-lb/in²Average value: 7.38 kJ/m² Grade Count:4
 6.00 - 6.00 kJ/m²
@Temperature -30.0 - -30.0 °C
2.86 - 2.86 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 6.00 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.00 - 8.60 J/cm²9.52 - 40.9 ft-lb/in²Average value: 4.65 J/cm² Grade Count:11
 1.70 - 3.00 J/cm²
@Temperature -30.0 - -20.0 °C
8.09 - 14.3 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 2.74 J/cm² Grade Count:3
Charpy Impact, Notched 0.350 - 1.10 J/cm²1.67 - 5.24 ft-lb/in²Average value: 0.642 J/cm² Grade Count:10
 0.400 - 0.600 J/cm²
@Temperature -40.0 - -20.0 °C
1.90 - 2.86 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.517 J/cm² Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1000 - 1.00e+16 ohm-cm1000 - 1.00e+16 ohm-cmAverage value: 2.01e+15 ohm-cm Grade Count:15
Surface Resistance 1000 - 1.00e+15 ohm1000 - 1.00e+15 ohmAverage value: 2.53e+14 ohm Grade Count:4
Dielectric Constant 3.90 - 5.203.90 - 5.20Average value: 4.30 Grade Count:6
Dielectric Strength 16.5 - 20.5 kV/mm419 - 520 kV/inAverage value: 19.1 kV/mm Grade Count:5
Dissipation Factor 0.00550 - 0.02300.00550 - 0.0230Average value: 0.0140 Grade Count:5
Comparative Tracking Index 550 - 600 V550 - 600 VAverage value: 571 V Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 22.0 - 36.0 µm/m-°C12.2 - 20.0 µin/in-°FAverage value: 28.6 µm/m-°C Grade Count:12
 11.0 - 190 µm/m-°C
@Temperature 55.0 - 250 °C
6.11 - 106 µin/in-°F
@Temperature 131 - 482 °F
Average value: 42.8 µm/m-°C Grade Count:9
CTE, linear, Transverse to Flow 59.0 - 96.0 µm/m-°C32.8 - 53.3 µin/in-°FAverage value: 73.4 µm/m-°C Grade Count:10
 100 - 160 µm/m-°C
@Temperature 55.0 - 250 °C
55.6 - 88.9 µin/in-°F
@Temperature 131 - 482 °F
Average value: 124 µm/m-°C Grade Count:8
Melting Point 300 - 325 °C572 - 617 °FAverage value: 312 °C Grade Count:12
Deflection Temperature at 0.46 MPa (66 psi) 220 - 318 °C428 - 604 °FAverage value: 284 °C Grade Count:14
Deflection Temperature at 1.8 MPa (264 psi) 161 - 277 °C322 - 531 °FAverage value: 245 °C Grade Count:26
Vicat Softening Point 215 - 275 °C419 - 527 °FAverage value: 246 °C Grade Count:5
Flammability, UL94 HB - V-0HB - V-0Grade Count:20
Oxygen Index 23.0 - 32.0 %23.0 - 32.0 %Average value: 29.0 % Grade Count:3
 
Optical PropertiesMetricEnglishComments
Reflection Coefficient, Visible (0-1) 0.9000.900Average value: 0.900 Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 296 - 340 °C565 - 644 °FAverage value: 315 °C Grade Count:4
Melt Temperature 240 - 343 °C464 - 650 °FAverage value: 322 °C Grade Count:26
Mold Temperature 65.0 - 180 °C149 - 356 °FAverage value: 127 °C Grade Count:28
Drying Temperature 90.0 - 130 °C194 - 266 °FAverage value: 109 °C Grade Count:23
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.0776 % Grade Count:19
Dew Point -31.7 - -28.9 °C-25.0 - -20.0 °FAverage value: -30.4 °C Grade Count:9
Injection Pressure 68.9 - 124 MPa10000 - 18000 psiAverage value: 93.1 MPa Grade Count:12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
Overview of materials for Polyphthalamide (PPA)
Overview of materials for Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced

O4612 / 78360

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.