MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Chemical Advanced Materials TIVAR™ Sterra™ UHMW-PE Recycled Ultra High Molecular Weight Polyethylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Recycled UHMW-PE shapes that exhibit excellent abrasion and corrosion resistance and are commonly used in wear and outrigger pads, strips, rails, guides, rollers, conveyors, chutes, hoppers, impact plates, and asphalt equipment components.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60.060.0ISO 868
Tensile Strength 20.0 MPa2900 psiISO 527-1/-2 (7)
Elongation at Yield 18.0 %18.0 %ISO 527-1/-2 (7)
Flexural Strength 18.0 MPa2610 psiISO 178 (12)
Compressive Yield Strength  6.00 MPa
@Strain 1.00 %
870 psi
@Strain 1.00 %
ISO 604 (10)
 9.00 MPa
@Strain 2.00 %
1310 psi
@Strain 2.00 %
ISO 604 (10)
 15.0 MPa
@Strain 5.00 %
2180 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 20.0 MPa2900 psiASTM D732
Charpy Impact, Notched 11.6 J/cm²55.2 ft-lb/in²Partial Break; ISO 179-1/1eA
 18.0 J/cm²85.7 ft-lb/in²Double Notched
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+13 ohm1.00e+13 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C
@Temperature 23.0 - 100 °C
111 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 82.2 °C180 °FContinuous Use Temperature in Air after 20000 hr
Minimum Service Temperature, Air -150 °C-238 °F
 -150 °C-238 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SMU790 / 323900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.