MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chosun Refractories SC80 Bricks, Oxide Bonded SiC
Categories: Ceramic; Carbide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.65 g/cc0.0957 lb/in³
Porosity 17 %17 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.024525 GPa
@Temperature 250 °C
3.5571 ksi
@Temperature 482 °F
 0.024525 GPa
@Temperature 1400 °C
3.5571 ksi
@Temperature 2550 °F
Compressive Strength 88.3 MPa12800 psiCold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.80 µm/m-°C
@Temperature 1000 °C
2.67 µin/in-°F
@Temperature 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 1.1 %1.1 %
SiC 81 %81 %
 
Descriptive Properties
Refractories Under Load(2kg/cm²,T2°C)1,600

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
China-Yixing Longly Refractories ASM-130 Cordierite-Mullite
Thermal Ceramics Firebrick SR-90
Thermal Ceramics Firebrick SR-99
China-Yixing Longly Refractories ASM-120 Cordierite-Mullite
Microtherm Group Slim&Light Fire Resistant Insulation

CCHOS057 / 124001

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.