MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® HHM TR-480X HDPE Pipe and Corrugated Extrusion Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Characteristics:
  • Good long-term hoop strength performance
  • Very high melt strength
  • Outstanding low temperature toughness

Applications:

  • Municipal, industrial, and mining pipe
  • Oil and gas gathering pipe

Information provided by Chevron Phillips.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D1505
Melt Flow 11 g/10 min11 g/10 minCondition 190/2.16, HLMI; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 100 hour>= 100 hourSlow crack growth; ASTM F1473
Tensile Strength, Yield 22.0 MPa3190 psi2 in/min, Type IV bar; ASTM D638
Elongation at Break 800 %800 %2 in/min, Type IV bar; ASTM D638
Flexural Modulus 0.960 GPa139 ksiTangent, 16:1 span:depth,0.5in/min; ASTM D790
 0.760 GPa
@Strain 2 %
110 ksi
@Strain 2 %
Secant; 16:1 span:depth, 0.5 in/min; ASTM D3350
Hydrostatic Design Basis 5.50 MPa798 psi60°C; ASTM D2837
 11.0 MPa
@Temperature 23.0 °C
1600 psi
@Temperature 73.4 °F
ASTM D2837
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -75.0 °C<= -103 °FType A clamp, type 1 specimen; ASTM D746
 
Descriptive Properties
Minimum Required Strength8 MPaISO 9080

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® C514 HDPE Pipe and Corrugated Extrusion Resin
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
ExxonMobil HD 56200 High Density Polyethylene Resin
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding
Chevron Phillips Marlex® 9519H High Density Polyethylene, Blow Molding

PCHEVD026 / 20639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.