MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group QSil 60 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting
Categories: Polymer; Thermoset; Silicone

Material Notes: QSil 60 is a red, high temperature, self-leveling, two-component, silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section Catalyst by weight. The 0.5% catalyst level can be increased or decreased to obtain desired cure speed. Cure speed can be accelerated by adding DBT catalyst in increments of 0.1%. QSil 60 can be catalyzed with 10% Deep Section Catalyst for application requiring a deeper cure. The material can also be vulcanized at elevated temperatures to increase cure speed.

Key Features:

  • Excellent thermal stability
  • Self-leveling
  • Variable cure speed
Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccuncatalyzed, DBT Catalyst
 1.47 g/cc1.47 g/ccuncatalyzed, Deep Section Catalyst
 1.48 g/cc1.48 g/cccatalyzed
 1.49 g/cc1.49 g/ccuncatalyzed
Viscosity 6500 cP6500 cPuncatalyzed, Deep Section Catalyst
 55000 cP55000 cP
Storage Temperature <= 4.00 °C<= 39.2 °F12 months
 5.00 - 27.0 °C41.0 - 80.6 °F3 months
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060catalyzed, 24 hours
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °Fcontinuously and up to 316°C (600°F) intermittently
Minimum Service Temperature, Air -54.0 °C-65.2 °F
 
Processing PropertiesMetricEnglishComments
Gel Time 45.0 min45.0 min
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QSil 940 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting
Wacker Silpuran® 8020/60 Silicone Rubber
Wacker Elastosil® R 701/60 Silicone Rubber
Shin-Etsu Silicones KE-9611U Silicone Elastomer
Precision Polymer Engineering S60R Silicone Rubber

PACC040 / 22167

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.