MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAFIL PPSU natural - 1,75 mm - Filament Polyphenylsulfone
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes:
  • high strength
  • inherent flame retardant
  • good chemical resistance
  • good heat deflection temperature
  • high thermal and mechanical capacity
Target Industries:
  • automotive industry
  • chemical technology
  • mechanical engineering
  • aircraft and aerospace interiors
  • aircraft and aerospace technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³
Moisture Absorption 0.600 %0.600 %DIN EN ISO 62
Melt Flow 35 g/10 min
@Load 10.0 kg,
Temperature 360 °C
35 g/10 min
@Load 22.0 lb,
Temperature 680 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 59.0 MPa8560 psi5mm/min, Orientation ZX; DIN EN ISO 527-2
 65.0 MPa9430 psi5mm/min, Orientation XY; DIN EN ISO 527-2
Elongation at Break 5.0 %5.0 %5mm/min, Orientation ZX; DIN EN ISO 527-2
 11.7 %11.7 %5mm/min, Orientation XY; DIN EN ISO 527-2
Modulus of Elasticity 1.92 GPa278 ksi5mm/min, Orientation XY; DIN EN ISO 527-2
 2.06 GPa299 ksi5mm/min, Orientation ZX; DIN EN ISO 527-2
Flexural Strength 85.0 MPa12300 psi2mm/min, Orientation ZX; DIN EN ISO 178
 91.0 MPa13200 psi2mm/min, Orientation XY; DIN EN ISO 178
Flexural Modulus 1.90 GPa276 ksi2mm/min, Orientation ZX; DIN EN ISO 178
 2.05 GPa297 ksi2mm/min, Orientation XY; DIN EN ISO 178
Flexural Strain at Break 5.7 %5.7 %2mm/min, Orientation ZX; DIN EN ISO 178
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C30.6 µin/in-°FDIN EN ISO 11359-1;2
Maximum Service Temperature, Air 170 °C338 °Flong term
 190 °C374 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 198 °C388 °FISO-R 75 Method A
Glass Transition Temp, Tg 220 °C428 °FASTM D3418
Flammability, UL94 V-0V-0125x13x1,5mm; DIN IEC 60695-11-10
 V-0V-0125x13x3mm; DIN IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 230 °C320 - 446 °FPrint bed temperature
 190 - 210 °C374 - 410 °FBuild chamber temperature
Nozzle Temperature 360 - 400 °C680 - 752 °FDiameter: 0,4 mm
Melt Temperature <= 410 °C<= 770 °F
Drying Temperature 120 °C248 °F
Dry Time 8.00 hour8.00 hour
 
Descriptive Properties
Coloramber transparent
Fan speed0
Flammability1.4 mm60 sec. Vertical Bunsen Burner test, FAR §25.853 (a) and Appendix F, Part I, para. (a)(1)(i)
 1.5 mm12 sec. Vertical Bunsen Burner test, FAR §25.853 (a) and Appendix F, Part I, para. (a)(1)(ii)
 1.5 mm15 sec. Horizontal Bunsen Burner test, FAR §25.853 (a) and Appendix F, Part I, para. (a)(1)(iv)
 1.5 mmHeat Release, as per FAR §25.853 (d) and Appendix F, Part IV
 1.5 mmSmoke density, as per FAR §25.853 (d) and Appendix F, Part V
 1.5 mmGas Toxicity, as per Boeing BSS 7239
Print speed30-40 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO1274 / 319202

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.