MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem Green PE SPB681 Injection Molded, Blown and Cast Film Low Density Polyethylene
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Description: SPB681 is a low density polyethylene produced under high pressure technology. Films obtained with this product show excellent 'draw down', good sealability, and low gel content. Additives free. The minimum biobased content of this grade is 95%, determined according to ASTM D6866.

Applications: LLDPE and HDPE blends.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ASTM D792
Melt Flow 3.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 370 %370 %ASTM D882
Film Elongation at Break, TD 1070 %1070 %ASTM D882
Elmendorf Tear Strength TD 100 g100 gASTM D1922
Dart Drop Test 60.0 g0.132 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 30.0 MPa4350 psiASTM D882
Film Tensile Strength at Break, TD 20.0 MPa2900 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %4.0 %ASTM D1003
Gloss 120 %120 %60°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 220 °C356 - 428 °FProfile, Injection
Zone 1 110 °C230 °FBlown Film Extrusion
Die Temperature 150 °C302 °FBlown Film Extrusion
 250 - 290 °C482 - 554 °FCast Film Extrusion
Mold Temperature 5.00 - 25.0 °C41.0 - 77.0 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Green PE SGF4950HS Blow Molded High Density Polyethylene
Braskem Green PE SGD4960 Blow Molded High Density Polyethylene
Braskem Green PE SEB853/72 Blown Film Extrusion Low Density Polyethylene
Braskem Green PE SEB853 Blown and Cast Film Extrusion Low Density Polyethylene
Braskem Green PE SBF0323HC Blown Film Extrusion Low Density Polyethylene

PBRASK2016 / 199898

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.