Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification). USES: Circuit breaker parts. Information provided by Vyncolit, a Sumitomo Bakelite Group |