MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Röchling LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Application: sheaves and wheels without additional bearings, sliding liners

Information provided by Schwartz Technical Plastics GmbH. Schwartz was acquired by Röchling in 2018.

Key Words: PA 6 G + Öl
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO R 1183
Moisture Absorption at Equilibrium 1.0 %1.0 %DIN 53473
Water Absorption at Saturation 4.0 %
@Temperature 20.0 °C
4.0 %
@Temperature 68.0 °F
ISO R 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 130 MPa18900 psiHc 30; ISO 2039; partially
Tensile Strength, Yield 70.0 MPa10200 psiISO-DIS 527
Creep Strength >= 12.0 MPa>= 1740 psi1% elongation, 1000 h; DIN 53444
 >= 16.0 MPa>= 2320 psi2% elongation, 1000 h; DIN 53444
Tensile Modulus 2.80 GPa406 ksiDIN 53457
Flexural Strength 60.0 MPa8700 psiDIN 54352
Flexural Modulus 2.50 GPa363 ksiDIN 53457
Compressive Strength 21.0 MPa3050 psi5% pressing; EN ISO 604
 43.0 MPa6240 psi10% pressing; EN ISO 604
 66.0 MPa9570 psi20% pressing; EN ISO 604
Izod Impact, Notched (ISO) >= 15.0 kJ/m²>= 7.14 ft-lb/in²ISO 180-1A
Izod Impact Resistance NBNBswinging hammer 0,1 DIN 51222; DIN 53453
Coefficient of Friction 0.0800.080With lubrication
Coefficient of Friction, Dynamic 0.200.20no lube; Steel 2162, Rvst=2E-6m, p=0.05 Mpa, v=0.6 m/s, t=40°C
Tear Strength Test >= 0.25>= 0.25ISO-DIS 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmDIN 53482
Surface Resistance 1.00e+10 ohm1.00e+10 ohmDIN 53482
Dielectric Constant 3.73.7DIN 53483
Dielectric Strength 20.0 kV/mm508 kV/inDIN 53481
Dielectric Loss Index 0.0300.030DIN 53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 - 80.0 µm/m-°C
@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F
@Temperature 68.0 - 212 °F
DIN 53752
Specific Heat Capacity 1.67 J/g-°C0.399 BTU/lb-°F
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FDIN 52612
Melting Point 220 °C428 °FISO R 1218
Maximum Service Temperature, Air 120 °C248 °FContinuous
 180 °C356 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FV-notch; ISO R 75
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FV-notch; ISO R 75
Minimum Service Temperature, Air -40.0 °C-40.0 °FContinuous
 
Descriptive Properties
Creepage/leakage ResistanceKA3bDIN 53480
Friction Wear0.04 micron/km

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Conditioned
Röchling LAMIGAMID® 1200 Cast Polyamide 12, Dry
Röchling LAMIGAMID® 100 Polyamide 6, Extruded, Dry
Röchling LAMIGAMID® 100 Polyamide 6, Extruded, Conditioned

PSCHW018 / 90215

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.