MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials AC6103 Boron Nitride (BN) Powder
Categories: Ceramic; Nitride; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Agglomerate of hexagonal BN crystals. AC6103 powders are granular with good flow and blend characteristics as well as high thermal conductivity and good lubrication qualities.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 g/cc0.0181 lb/in³Tap Density
Particle Size 250 µm250 µm
Specific Surface Area 6.5 m²/g6.5 m²/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials AC6041 Boron Nitride (BN) Powder
Momentive Performance Materials AC6069 Boron Nitride (BN) Powder
Momentive Performance Materials AC6001 Boron Nitride (BN) Powder
Momentive Performance Materials AC6003 Boron Nitride (BN) Powder
Momentive Performance Materials AC6097 Boron Nitride (BN) Powder

CADV11e / 149813

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.