MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Dipolen™ S-74 Polyolefin, post-consumer recycled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyolefin

Material Notes: Dipolen" S-74 is a dark grey polyolefin (polypropylene/polyethylene blend) post-consumer recycled (rPO) supplied in different colors. This product is an ideal PO used where sustainability and circularity matter. Dipolen" S-74 is a post-consumer recycled including a large part of recycled post-consumer waste coming from pre-sorted household waste. It is part of the EuCertPlast certificate according to the European Standard EN15343:2007 (certificate available upon request). Due to the nature of recycleds, some variation in color can be observed between batches.
  • Good demolding properties
  • Filtration: 180 ¼m
  • Available in homogenized 24-ton truckloads
Applications: Extrusion and injection molding applications

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ISO 1183
Melt Flow 6.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash <= 5.00 %
@Treatment Temp. 950 °C
<= 5.00 %
@Treatment Temp. 1740 °F
ISO 1172
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.0 MPa3190 psi50 mm/min; ISO 527-2
Tensile Modulus 0.900 GPa131 ksi1 mm/min; ISO 527-2
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179-1/1eA
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 260 °C410 - 500 °F
Mold Temperature 30.0 - 40.0 °C86.0 - 104 °F
Moisture Content <= 0.100 %<= 0.100 %
Hold Pressure 20.0 - 50.0 MPa2900 - 7250 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9733 / 323090

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.