MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CHT AS1622 RTV, silicone adhesive sealant
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Description: This is a 1-part, RTV (Room Temperature Vulcanizing) silicone adhesive sealant. It is one in a range of Oxime cure products which are solvent free. It exhibits good primerless adhesion to many substrates especially plastics and cures rapidly at room temperature when in contact with atmospheric moisture. This product can be described as low corrosive but would not be recommended for use with copper or its associated alloys.

Key Features

  • Excellent flow and self leveling properties
  • Low corrosion
  • Good adhesion to substrates
Cured Product: 7 days at 23+/-2°C and 50+/-5% humidity

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³BS ISO 2781
Brookfield Viscosity 23500 cP23500 cPMixed
Linear Mold Shrinkage 0.010 cm/cm0.010 in/in
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2424ASTM D2240-95
Tensile Strength 1.90 MPa276 psiISO 37
Elongation at Break 390 %390 %ISO 37
Tensile Modulus 0.000552 GPa0.0800 ksiYoung's
100% Modulus 0.317 MPa46.0 psi
Tear Strength 3.16 kN/m18.0 pliBS ISO 34-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D-257
Dielectric Constant 2.62.6ASTM D-150
Dissipation Factor 0.00100.0010ASTM D-150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 282 µm/m-°C157 µin/in-°F
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 275 °C527 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Extrusion Rate 860 g/min860 g/min
Cure Time 13.0 min0.217 hourTack Free Time / Skin Formation
 <= 1440 min
@Temperature 23.0 °C
<= 24.0 hour
@Temperature 73.4 °F
3mm Depth
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceViscous liquid
ColorBlack
Cure typeOxime
RheologyFlowable
Volume Coefficient of Thermal Expansion846 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL018 / 314501

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.