MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior ForTii® XS51 PPA-GF FR(40) PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

ForTii® XS51 offers an excellent balance of mechanical strength and flow. Its stable process behavior can allow high quality surface requirements such as Notebook covers. XS51 can support complicated geometry design and enabling robust mechanical performance in drop test. Features: Phosphorous free. 50% glass reinforced. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.67 g/cc0.0603 lb/in³Dry; ISO 1183
Moisture Absorption 1.50 %1.50 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0038 cm/cm0.0038 in/inDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0059 cm/cm0.0059 in/inDry; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 210 MPa30500 psiCond; ISO 527-1/-2
 230 MPa33400 psiDry; ISO 527-1/-2
Elongation at Break 2.0 %2.0 %Cond; ISO 527-1/-2
 2.3 %2.3 %Dry; ISO 527-1/-2
Tensile Modulus 18.5 GPa2680 ksiDry; ISO 527-1/-2
 19.0 GPa2760 ksiCond; ISO 527-1/-2
Flexural Strength 310 MPa45000 psiCond; ISO 178
 350 MPa50800 psiDry; ISO 178
Flexural Modulus 17.0 GPa2470 ksiDry; ISO 178
 18.0 GPa2610 ksiCond; ISO 178
Charpy Impact Unnotched  7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
Cond; ISO 179/1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
Cond; ISO 179/1eA
 1.35 J/cm²
@Temperature 23.0 °C
6.42 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 30.0 kV/mm762 kV/inDry; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 45.0 µm/m-°C25.0 µin/in-°FDry; ISO 11359-1/-2
CTE, linear, Parallel to Flow 15.0 µm/m-°C8.33 µin/in-°FDry; ISO 11359-1/-2
Melting Point 315 °C599 °F10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FDry; ISO 75-1/-2
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Dry; IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSM7937 / 291373

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.