MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Gold Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Gold Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.18 - 19.9 g/cc0.259 - 0.720 lb/in³Average value: 15.2 g/cc Grade Count:141
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 25.0 - 16925.0 - 169Average value: 88.2 Grade Count:6
Hardness, Knoop 131 - 2300131 - 2300Average value: 694 Grade Count:4
Hardness, Rockwell A 40.0 - 53.040.0 - 53.0Average value: 45.7 Grade Count:3
Hardness, Rockwell B 64.0 - 86.064.0 - 86.0Average value: 74.3 Grade Count:3
Hardness, Rockwell 15T 61.0 - 91.061.0 - 91.0Average value: 77.2 Grade Count:6
Hardness, Vickers 25.0 - 106025.0 - 1060Average value: 177 Grade Count:67
Tensile Strength, Ultimate 120 - 1900 MPa17400 - 276000 psiAverage value: 449 MPa Grade Count:83
Tensile Strength, Yield 80.0 - 907 MPa11600 - 132000 psiAverage value: 457 MPa Grade Count:56
Elongation at Break 1.20 - 56.5 %1.20 - 56.5 %Average value: 20.6 % Grade Count:84
Modulus of Elasticity 59.1 - 279 GPa8570 - 40500 ksiAverage value: 104 GPa Grade Count:40
Compressive Yield Strength 128 - 758 MPa18600 - 110000 psiAverage value: 514 MPa Grade Count:4
Poissons Ratio 0.210 - 0.4200.210 - 0.420Average value: 0.378 Grade Count:6
Shear Modulus 26.2 - 28.1 GPa3800 - 4080 ksiAverage value: 27.4 GPa Grade Count:4
Shear Strength 185 - 276 MPa26800 - 40000 psiAverage value: 227 MPa Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000220 - 0.0000620 ohm-cm0.00000220 - 0.0000620 ohm-cmAverage value: 0.0000175 ohm-cm Grade Count:57
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.90 - 19.5 µm/m-°C2.72 - 10.8 µin/in-°FAverage value: 15.1 µm/m-°C Grade Count:61
Specific Heat Capacity 0.128 - 0.150 J/g-°C0.0306 - 0.0359 BTU/lb-°FAverage value: 0.133 J/g-°C Grade Count:7
Thermal Conductivity 21.0 - 301 W/m-K146 - 2090 BTU-in/hr-ft²-°FAverage value: 64.7 W/m-K Grade Count:33
Melting Point 280 - 1880 °C536 - 3410 °FAverage value: 915 °C Grade Count:179
Solidus 280 - 1290 °C536 - 2350 °FAverage value: 869 °C Grade Count:165
Liquidus 280 - 1450 °C536 - 2640 °FAverage value: 927 °C Grade Count:165
 
Optical PropertiesMetricEnglishComments
Reflection Coefficient, Visible (0-1) 0.270 - 0.8500.270 - 0.850Average value: 0.695 Grade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 315 - 1230 °C599 - 2250 °FAverage value: 746 °C Grade Count:73
Casting Temperature 950 - 1430 °C1740 - 2610 °FAverage value: 1160 °C Grade Count:50
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd 0.00100 %0.00100 %Average value: 0.00100 % Grade Count:8
Carbon, C 0.00500 - 0.0100 %0.00500 - 0.0100 %Average value: 0.00714 % Grade Count:7
Cobalt, Co 0.0600 - 0.800 %0.0600 - 0.800 %Average value: 0.520 % Grade Count:3
Copper, Cu 0.000 - 97.0 %0.000 - 97.0 %Average value: 21.1 % Grade Count:87
Germanium, Ge 12.0 %12.0 %Average value: 12.0 % Grade Count:5
Gold, Au 3.00 - 100 %3.00 - 100 %Average value: 69.2 % Grade Count:190
Indium, In 0.200 - 25.0 %0.200 - 25.0 %Average value: 4.73 % Grade Count:31
Iridium, Ir 0.100 - 0.300 %0.100 - 0.300 %Average value: 0.122 % Grade Count:27
Iron, Fe 0.200 - 1.00 %0.200 - 1.00 %Average value: 0.400 % Grade Count:4
Lead, Pb 0.00200 %0.00200 %Average value: 0.00200 % Grade Count:8
Manganese, Mn 6.80 - 16.0 %6.80 - 16.0 %Average value: 10.2 % Grade Count:4
Nickel, Ni 1.15 - 36.5 %1.15 - 36.5 %Average value: 18.0 % Grade Count:40
Palladium, Pd 1.00 - 76.0 %1.00 - 76.0 %Average value: 12.7 % Grade Count:54
Phosphorus, P 0.00200 - 0.200 %0.00200 - 0.200 %Average value: 0.0268 % Grade Count:8
Platinum, Pt 0.400 - 30.0 %0.400 - 30.0 %Average value: 9.15 % Grade Count:39
Rhenium, Re 0.100 %0.100 %Average value: 0.100 % Grade Count:10
Rhodium, Rh 0.500 - 0.700 %0.500 - 0.700 %Average value: 0.533 % Grade Count:6
Silicon, Si 2.00 - 3.20 %2.00 - 3.20 %Average value: 2.78 % Grade Count:3
Silver, Ag 0.500 - 59.2 %0.500 - 59.2 %Average value: 17.5 % Grade Count:89
Tin, Sn 0.100 - 22.0 %0.100 - 22.0 %Average value: 14.0 % Grade Count:12
Zinc, Zn 0.00100 - 14.5 %0.00100 - 14.5 %Average value: 5.65 % Grade Count:55

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Grade 2
Titanium Grade 4
Titanium Alloys, General
Titanium Grade 1
Overview of materials for Silver Alloy

M01063 / 81694

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.