MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Donnelly Bros HT 500 High Temperature Mold Grease
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE); PTFE Gellant

Material Notes: White. Slight odor. Use caution when handling. Light caramel-like texture. Does not migrate, works well in constant metal temperature of 250° F to 500° F. (Note: The plastic molding material itself might be much higher temperature.)

A stiff, PTFE thickened, medium viscosity, completely fluorinated grease possessing very wide temperature capability, excellent plastic and elastomer compatibility and resistance to aggressive chemicals.

Information provided by Donnelly Bros. Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.88 g/cc0.0679 lb/in³ASTM D1480
Viscosity 1.70e+6 cP1.70e+6 cP
Viscosity Measurement 136136Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 345 cSt345 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 33 cSt33 cStASTM D445
Evaporation Loss 0.30 %0.30 %150°C; 22 hrs
 
Mechanical PropertiesMetricEnglishComments
Penetration P(0), 1/10 mm 230230ASTM D217
Penetration P(60), 1/10 mm 239239ASTM D217
Oil Separation 3.0 %3.0 %150°C; 22 hrs; FTM 791B, 321.2
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Pour Point -25.0 °C-13.0 °FUniFlor 8610 Base Oil; ASTM D97
 
Descriptive Properties
AppearanceSmooth
Base OilUniFlor 8610
ColorWhite
NLGI Grade3ASTM D217

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Krytox® LVP High-Vacuum Grease
Chemours Krytox® 16530 Vacuum Service Fluid

WDONNEL2 / 75356

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.