MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Gharda Chemicals GAFONE™-S 20% Glass Fiber-Reinforced PSU, High Thermal Stability  (discontinued **)
Categories: Polymer; Thermoplastic; Polysulfone (PSU); Polysulfone, 20% Glass Fiber Reinforced

Material Notes: Characteristics:
  • Good dielectric properties
  • High mechanical strength
  • Good dimensional stability
  • Good oxidative stability
  • Inherent flame retardance
  • Good hydrolytic stability

Applications:

  • Printer cartridges
  • Mobile phone parts
  • Surgical tool trays
  • Dental cases
  • Business machine parts
  • Alkaline battery cell cases
  • Household appliances

Information provided by Gharda.

Solvay Advanced Polymers completed its acquisition of this product line in May 2006.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Filler Content 20 %20 %
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa16700 psiISO 527
Elongation at Break 2.0 %2.0 %ISO 527
Tensile Modulus 7.00 GPa1020 ksiISO 527
Flexural Strength 150 MPa21800 psiISO 178
Flexural Modulus 6.70 GPa972 ksiISO 178
Izod Impact, Notched 0.650 J/cm1.22 ft-lb/inISO 170
Izod Impact, Unnotched 3.35 J/cm6.28 ft-lb/inISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 93
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 93
Dielectric Strength 20.0 kV/mm508 kV/inIEC 243/1
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 165 °C329 °FContinuous use, UL
Deflection Temperature at 1.8 MPa (264 psi) 183 °C361 °FISO 75
Glass Transition Temp, Tg 185 °C365 °FDSC
Flammability, UL94 V-0
@Thickness 4.50 mm
V-0
@Thickness 0.177 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fulcrum Composites Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Rod
Avient Edgetek® PF-1000 Polysulfone
Avient Stat-Tech™ PF-05CF/000 EM FR Flame Retardant Polysulfone - 5% Carbon Fiber
Overview of materials for Polyethersulfone (PES)
Overview of materials for Polycarbonate, Extruded

PGHARDA11 / 41786

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.