MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zircar Zirconia HfF-15 Hafnia Knit Textile Insulation
Categories: Ceramic; Machinable Ceramic; Oxide

Material Notes: Our hafnia (HfO2) fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia cloths and felts. Our high purity hafnia fiber and textiles are offered in six different standard product forms; bulk fiber Type HfBF, two felts Types HfF-50 and HfF-100 and three types of knit cloth Types HfK-15, HfW-15 and HfW- 30.

Features:

  • High Purity
  • High Temperature Stability
  • Low Thermal Conductivity
  • Excellent Thermal Shock Resistance
  • No Outgassing
  • Six Different Product Formats Offered
  • Available ‘Off the Shelf’

Application Information:

  • Hafnia is used as ultra high temperature insulation for nuclear meltdown experiments.

Information provided by Zircar Zirconia.

Key Words: HfO2, hafnium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.10 g/cc0.0397 lb/in³
Loss On Ignition 0.00 %
@Temperature 950 °C,
Time 3600 sec
0.00 %
@Temperature 1740 °F,
Time 1.00 hour
Porosity 89 %89 %Bulk
Outgassing - Total Mass Loss 0.00 %0.00 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 2758 °C4996 °F
Shrinkage 6.0 %
@Temperature 1650 °C,
Time 3600 sec
6.0 %
@Temperature 3000 °F,
Time 1.00 hour
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 0.012 %0.012 %
HfO2 >= 99 %>= 99 %
SiO2 <= 0.010 %<= 0.010 %
ZrO2 0.026 %0.026 %
 
Descriptive Properties
Tensile Strength per Unit Width100 gram/cm width

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hafnium (II) Oxide, HfO2 (Hafnia)
Zircar Zirconia HfF-100 Hafnia Felt Insulation
Hafnium Oxide, HfO2
American Elements Hafnium Oxide Nanopowder
Anderman Ceramics EREH99 Hafnium Oxide, High Purity

C6ZIR033 / 2789

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.