MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Envalior Stanyl® TE250F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Flame Retarded + Glass Fiber Reinforced

Material Notes: Information provided by DSM Engineering Plastics.

Former DSM Engineering Plastics product line is now with Envalior.

Key Words: Polyamide 46
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.6 %1.6 %50% RH / 23°C; Similar to ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 180 MPa26100 psiISO 527-1/-2
Elongation at Break 2.5 %2.5 %ISO 527-1/-2
Tensile Modulus 12.0 GPa1740 ksiISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179/1eU
 5.00 J/cm²
@Temperature -30.0 °C
23.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243-1
Comparative Tracking Index 250 V250 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 20.0 °C
11.1 µin/in-°F
@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 295 °C563 °FISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FISO 75-1/-2
UL RTI, Electrical 140 °C
@Thickness 1.50 mm
284 °F
@Thickness 0.0591 in
UL746B
Flammability, UL94 V-0
@Thickness 0.350 mm
V-0
@Thickness 0.0138 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DSM Stanyl® ForTii™ F11C PA4T-GF30 FR (40), Dry, 30% Glass Filled, Flame Retardant
Celanese Zenite® 6130 BK010 LCP, 30% glass reinforced (Extended Tabular Temperature Data)
Celanese VECTRA E115i LCP, 15% Glass Reinforced
Celanese Thermx® CG933 NC010 PCT
Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced

PDSMA016 / 30950

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.