MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Baydur® 426 IMR RIM system
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Solid RIM

Material Notes: Characterization: Baydur 426 IMR is a polyurethane high density structural RIM (HD SRIM) system.

Properties / Applications: Baydur 426 IMR is a polyurethane high density structural RIM (HD SRIM) system used for automotive and light truck applications. This system is well suited for load bearing truck beds, tailgates, bumper beams, load floors, etc. It has excellent heat stability performance. Baydur 426 IMR composites can be used to replace steel or structural plastics for significant weight reduction ad lower tooling costs. Due to its inherent nature, this system is corrosion and abrasion resistant. The Baydur 426 IMR system can be processed with either a closed mold or open mold. This system is combined with a variety of glass reinforcements to make a structural composite. Glass mats, directed chop preforms or glass rovings can be used for reinforcement. This system has the appropriate reaction rate so that it can be used with a chopped glass fiber RIM machine. The Baydur 426 IMR system has an exceptionally long gel time, yet fast cure time, that makes it well suited for large automotive parts.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccPolyol (Component B)
 1.24 g/cc1.24 g/ccIsocyanate (Component A)
 1.50 g/cc1.50 g/ccContinuous filament mat; ASTM D792
 1.65 g/cc1.65 g/ccChopped glass preform; ASTM D792
Viscosity 200 cP200 cPIsocyanate (Component A)
 2150 cP2150 cPPolyol (Component B)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 180 MPa26100 psiContinuous filament mat; ASTM D638
 188 MPa27300 psiChopped glass preform; ASTM D638
Flexural Strength 300 MPa43500 psiContinuous filament mat; ASTM D790
 315 MPa45700 psiChopped glass preform; ASTM D790
Flexural Modulus 10.5 GPa1520 ksiChopped glass preform; ASTM D790
 11.5 GPa1670 ksiContinuous filament mat; ASTM D790
 
Thermal PropertiesMetricEnglishComments
CTE, linear 27.0 µm/m-°C15.0 µin/in-°FContinuous filament mat; ASTM D696
 30.6 µm/m-°C17.0 µin/in-°FChopped glass preform; ASTM D696
Flash Point 186 °C367 °FPMCC, Polyol (Component B)
 199 °C390 °FPMCC, Isocyanate (Component A)
 
Processing PropertiesMetricEnglishComments
Mold Temperature 80.0 - 100 °C176 - 212 °F
Gel Time 15.0 - 20.0 min15.0 - 20.0 min
 
Descriptive Properties
AppearanceBlack liquidPolyol (Component B)
 Dark brown liquidIsocyanate (Component A)
Content>31%NCO, Isocyanate (Component A)
Hydroxyl numberPolyol (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Baydur® 263 IMR RIM system
Covestro Baypreg® F 310 Polyurethane, 10 mm
Covestro Prism® CM-200 Polyurethane Solid RIM, MDI-based 2-Component Liquid System
Coastal Enterprises Plus™ PBLT-75 High Density Urethane Foam
Celanese Zytel® FR70M30V0 BK010 PA66-MD30FR(17)

PCOVEST0080 / 201863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.