MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: KaMin® HG90 is a high brightness, ultra-fine particle size, platy kaolin with moderate water demand providing good tinting strength, Ti02 extension and gloss in water based paints. KaMin® HG90 is ideally suited for water-borne paint and ink applications, where high brightness and whiteness are important.

Industry: Paint & Coatings, Adhesives & Sealants, Ink

Uses: Architectural Coatings, Industrial Coatings, Wood Coatings, Satin, Gloss, Water Based, Gravure Water Based, Flexo Water Based

Information provided by KaMin LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.60 g/cc2.60 g/cc
Bulk Density 0.801 - 0.897 g/cc0.0289 - 0.0324 lb/in³Loose
Solids Content 69.5 - 71 %69.5 - 71 %Slurry
Brightness 90 - 91.5 %90 - 91.5 %Reflectance (TAPPI)
Oil Absorption 42 %42 %
Fineness >= 5>= 5Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %<= 1.5 %As Produced
Particle Size 0.20 µm0.20 µmAverage Stokes Equivalent Diameter
 0.40 µm0.40 µmMedian (Malvern Laser)
Particle Mesh Size 325 Mesh325 Mesh0.005% Retained
pH 6 - 86 - 8100 g/250 ml H2O Slurry
Specific Surface Area 21 m²/g21 m²/gBET
Brookfield Viscosity 450 cP
@Temperature 25.0 °C
450 cP
@Temperature 77.0 °F
20 RPM
 
Descriptive Properties
Bulking Value21.7 lb.gal
CAS Number1332-58-7
Crystalline Silica (quartz)<0.1%
Physical FormsDry, Slurry
Shipping PointWrens, GA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
KaMin KaMin® 100C Kaolin Clay - Calcined
KaMin KaMin® 70C Kaolin Clay - Calcined
KaMin Polygloss® 90 Kaolin Clay - Ultrafine, high brightness
Omya OMYACARB® UF - FL Calcium Carbonate
KaMin KaMin® HG Kaolin Clay - Waterwashed

CKAMAN925 / 178396

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.