MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermal Transfer Composites PRIMEX™ MCX-693™ Aluminum Silicon Carbide Composite, Reinforced
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy

Material Notes: Applications: Printed Wiring Board Cores; Carriers and Packaged Bases

Information provided by Thermal Transfer Composites

Key Words: AlSiC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.98 g/cc0.108 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 255 GPa37000 ksi
Flexural Strength 300 MPa43500 psi4 pt. bend
Poissons Ratio 0.240.24
Shear Modulus 103 GPa14900 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000300 - 0.0000500 ohm-cm0.0000300 - 0.0000500 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.30 µm/m-°C3.50 µin/in-°F
Specific Heat Capacity 0.720 - 0.760 J/g-°C
@Temperature 25.0 °C
0.172 - 0.182 BTU/lb-°F
@Temperature 77.0 °F
Thermal Conductivity 180 W/m-K
@Temperature 25.0 °C
1250 BTU-in/hr-ft²-°F
@Temperature 77.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Thermal Transfer Composites PRIMEX ULTRA™ MCT-487™ Aluminum Silicon Carbide Composite, Reinforced
Thermal Transfer Composites PRIMEX ULTRA™ MCT-587™ Aluminum Silicon Carbide Composite, Reinforced
Thermal Transfer Composites PRIMEX™ MCX-703™ Aluminum Silicon Carbide Composite, Reinforced
Thermal Transfer Composites PRIMEX™ MCX724™ Aluminum Silicon Carbide Composite, Reinforced
Thermal Transfer Composites PRIMEX Cast™ MCX-1195™ Aluminum Silicon Carbide Composite, Reinforced

CTTRAN01 / 122057

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.