MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Incusil™ Mac-Incusil™ ABA-WM Braze Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: High-purity Active Braze Alloy of silver, copper, indium and titanium, developed for direct application to ceramic surfaces.

Applications: High-integrity brazed joint duties for:

  • Vacuum tubes
  • Wave guide and Klystron assemblies

information provided by Morgan Advanced Materials

Key Words: Braze Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.69 g/cc0.350 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 10001000expressed as Mpa
Tensile Strength 455 MPa66000 psi
Elongation at Break 21 %21 %2 in/50mm gage section
Modulus of Elasticity 76.0 GPa11000 ksi
Compressive Yield Strength 338 MPa49000 psi0.2% offset
Poissons Ratio 0.360.36calculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000106 ohm-cm0.0000106 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.2 µm/m-°C
@Temperature 20.0 - 400 °C
10.1 µin/in-°F
@Temperature 68.0 - 752 °F
Thermal Conductivity 70.0 W/m-K486 BTU-in/hr-ft²-°Fcalculated
Melting Point 605 - 715 °C1120 - 1320 °F
Solidus 605 °C1120 °F
Liquidus 715 °C1320 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 715 - 740 °C1320 - 1360 °FBrazing Temperature
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd <= 0.0010 %<= 0.0010 %
Carbon, C <= 0.010 %<= 0.010 %
Chromium, Cr 14 %14 %nominal
Copper, Cu 27.25 %27.25 %nominal
Indium, In 12.5 %12.5 %nominal
Lead, Pb <= 0.0020 %<= 0.0020 %
Phosphorus, P <= 0.0020 %<= 0.0020 %
Silver, Ag 59 %59 %nominal
Titanium, Ti 1.25 %1.25 %nominal
Zinc, Zn <= 0.0010 %<= 0.0010 %
 
Descriptive Properties
Recommended Brazing Atmosphere1E-05(or inert gas) mm Hg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Cusil™ Mac-Cusil™-WM Braze Alloy
Morgan Advanced Ceramics Nioro™ ABA Mac-Nioro™ABA-WM Braze Alloy
Morgan Advanced Ceramics Palcusil™ Mac-Palcusil™10-WM Braze Alloy
Thermal Transfer Composites PRIMEX™ MCX-693™ Aluminum Silicon Carbide Composite, Reinforced
Morgan Advanced Ceramics Mac-35 Au/65 Cu-WM Braze Alloy

CMORF8009 / 203486

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.