MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

World Minerals Celite® Super Fine® Super Floss Diatomaceous Earth Antiblock Additive
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.

Antiblocking is accomplished via the varied particle shapes of diatomite particles that protrude from, or are at the surface of, the polyethylene film. The amount of Celite® antiblock required is generally in the 0.2% to 0.5% range.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.30 g/cc2.30 g/cc
Brightness 90 %90 %Blue Light
Particle Size 5.2 µm5.2 µmMedian
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.481.48
 
Component Elements PropertiesMetricEnglishComments
Al2O3 2.7 %2.7 %
CaO 0.10 %0.10 %
Fe2O3 0.90 %0.90 %
H2O, Water <= 0.50 %<= 0.50 %As Shipped
K2O+Na2O 3.3 %3.3 %
MgO 0.60 %0.60 %
SiO2 91.6 %91.6 %
 
Descriptive Properties
Hunter b Color Value<2Dry
 4.2Wet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
World Minerals Celite® White Mist® PF Diatomaceous Earth Antiblock Additive
World Minerals Celite® Super Floss® Diatomaceous Earth Antiblock Additive
BNZ Materials CS85 High Temperature Structural Insulation
Aptek 6512-PMF Electronic grade, conductive epoxy adhesive
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (CS Type B), Standard Grade

CCELIT90 / 97766

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.