MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior ForTii® MX15HR PPA-GF35 PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

ForTii® MX15HR exhibits enhanced hydrolytic stability towards aggressive coolants (water/glycol, 135°C) that are used in engine's thermal management systems. It has excellent mechanical performance and weld-line resistance. Features: Hydrolysis resistant or enhanced hydrolytic stability. 35% glass reinforced. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³Dry; ISO 1183
Moisture Absorption 2.00 %2.00 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0035 cm/cm0.0035 in/inDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0105 cm/cm0.0105 in/inDry; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  55.0 MPa
@Temperature 200 °C
7980 psi
@Temperature 392 °F
ISO 527-1/-2
 63.0 MPa
@Temperature 180 °C
9140 psi
@Temperature 356 °F
ISO 527-1/-2
 68.0 MPa
@Temperature 120 °C
9860 psi
@Temperature 248 °F
Cond; ISO 527-1/-2
 76.0 MPa
@Temperature 100 °C
11000 psi
@Temperature 212 °F
Cond; ISO 527-1/-2
 78.0 MPa
@Temperature 160 °C
11300 psi
@Temperature 320 °F
ISO 527-1/-2
 80.0 MPa
@Temperature 150 °C
11600 psi
@Temperature 302 °F
ISO 527-1/-2
 145 MPa
@Temperature 120 °C
21000 psi
@Temperature 248 °F
Dry; ISO 527-1/-2
 170 MPa
@Temperature 100 °C
24700 psi
@Temperature 212 °F
Dry; ISO 527-1/-2
 190 MPa
@Temperature 80.0 °C
27600 psi
@Temperature 176 °F
Dry; ISO 527-1/-2
 220 MPa
@Temperature 23.0 °C
31900 psi
@Temperature 73.4 °F
Cond; ISO 527-1/-2
 220 MPa
@Temperature 40.0 °C
31900 psi
@Temperature 104 °F
Dry; ISO 527-1/-2
 240 MPa
@Temperature 23.0 °C
34800 psi
@Temperature 73.4 °F
Dry; ISO 527-1/-2
 260 MPa
@Temperature -40.0 °C
37700 psi
@Temperature -40.0 °F
Dry; ISO 527-1/-2
Elongation at Break  2.4 %
@Temperature 23.0 °C
2.4 %
@Temperature 73.4 °F
Cond; ISO 527-1/-2
 2.5 %
@Temperature 40.0 °C
2.5 %
@Temperature 104 °F
Dry; ISO 527-1/-2
 2.6 %
@Temperature 23.0 °C
2.6 %
@Temperature 73.4 °F
Dry; ISO 527-1/-2
 2.6 %
@Temperature 80.0 °C
2.6 %
@Temperature 176 °F
Dry; ISO 527-1/-2
 2.7 %
@Temperature -40.0 °C
2.7 %
@Temperature -40.0 °F
Dry; ISO 527-1/-2
 2.7 %
@Temperature 100 °C
2.7 %
@Temperature 212 °F
Dry; ISO 527-1/-2
 2.8 %
@Temperature 120 °C
2.8 %
@Temperature 248 °F
Dry; ISO 527-1/-2
 6.3 %
@Temperature 120 °C
6.3 %
@Temperature 248 °F
Cond; ISO 527-1/-2
 6.6 %
@Temperature 100 °C
6.6 %
@Temperature 212 °F
Cond; ISO 527-1/-2
 8.0 %
@Temperature 150 °C
8.0 %
@Temperature 302 °F
ISO 527-1/-2
 8.0 %
@Temperature 160 °C
8.0 %
@Temperature 320 °F
ISO 527-1/-2
 8.0 %
@Temperature 180 °C
8.0 %
@Temperature 356 °F
ISO 527-1/-2
 8.0 %
@Temperature 200 °C
8.0 %
@Temperature 392 °F
ISO 527-1/-2
Tensile Modulus  3.70 GPa
@Temperature 200 °C
537 ksi
@Temperature 392 °F
ISO 527-1/-2
 4.00 GPa
@Temperature 180 °C
580 ksi
@Temperature 356 °F
ISO 527-1/-2
 4.60 GPa
@Temperature 120 °C
667 ksi
@Temperature 248 °F
Dry; ISO 527-1/-2
 4.60 GPa
@Temperature 160 °C
667 ksi
@Temperature 320 °F
ISO 527-1/-2
 5.00 GPa
@Temperature 100 °C
725 ksi
@Temperature 212 °F
Dry; ISO 527-1/-2
 5.30 GPa
@Temperature 150 °C
769 ksi
@Temperature 302 °F
ISO 527-1/-2
 11.2 GPa
@Temperature 120 °C
1620 ksi
@Temperature 248 °F
Dry; ISO 527-1/-2
 11.6 GPa
@Temperature 100 °C
1680 ksi
@Temperature 212 °F
Dry; ISO 527-1/-2
 11.9 GPa
@Temperature 80.0 °C
1730 ksi
@Temperature 176 °F
Dry; ISO 527-1/-2
 12.2 GPa
@Temperature 40.0 °C
1770 ksi
@Temperature 104 °F
Dry; ISO 527-1/-2
 12.5 GPa
@Temperature 23.0 °C
1810 ksi
@Temperature 73.4 °F
Dry; ISO 527-1/-2
 12.5 GPa
@Temperature -40.0 °C
1810 ksi
@Temperature -40.0 °F
Dry; ISO 527-1/-2
 12.9 GPa
@Temperature 23.0 °C
1870 ksi
@Temperature 73.4 °F
Cond; ISO 527-1/-2
Flexural Strength 290 MPa42100 psiCond; ISO 178
 320 MPa46400 psiDry; ISO 178
Flexural Modulus  3.70 GPa
@Temperature 200 °C
537 ksi
@Temperature 392 °F
ISO 178
 3.90 GPa
@Temperature 180 °C
566 ksi
@Temperature 356 °F
ISO 178
 4.30 GPa
@Temperature 160 °C
624 ksi
@Temperature 320 °F
ISO 178
 10.9 GPa
@Temperature 120 °C
1580 ksi
@Temperature 248 °F
ISO 178
 12.0 GPa
@Temperature 23.0 °C
1740 ksi
@Temperature 73.4 °F
Dry; ISO 178
 12.5 GPa
@Temperature 23.0 °C
1810 ksi
@Temperature 73.4 °F
Cond; ISO 178
Charpy Impact Unnotched  6.30 J/cm²
@Temperature -30.0 °C
30.0 ft-lb/in²
@Temperature -22.0 °F
Cond; ISO 179/1eU
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
Cond; ISO 179/1eU
 7.20 J/cm²
@Temperature -30.0 °C
34.3 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 7.60 J/cm²
@Temperature 23.0 °C
36.2 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
Cond; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Cond; ISO 179/1eA
 1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmDry; IEC 60093
 >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmCond; IEC 60093
Dielectric Strength 35.0 kV/mm889 kV/inDry; IEC 60243-1
 35.0 kV/mm889 kV/inCond; IEC 60243-1
Comparative Tracking Index 600 V600 VDry; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 51.0 µm/m-°C28.3 µin/in-°FDry; ISO 11359-1/-2
CTE, linear, Parallel to Flow 16.0 µm/m-°C8.89 µin/in-°FDry; ISO 11359-1/-2
Melting Point 330 °C626 °F10°C/min. Dry; ISO 11357-1/-3
Maximum Service Temperature, Air 170 °C338 °FThermal Index; 5000 hrs.; IEC 60216/ISO 527-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 300 °C572 °FDry; ISO 75-1/-2
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Dry; IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSM7917 / 291353

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.