MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

Westlake Plastics TPX® Polymethylpentene
Categories: Polymer; Thermoplastic; Polymethylpentene (PMP); Polymethylpentene, Molded

Material Notes: TPX™ Polymethylpentene (PMP) is a unique semi-crystalline thermoplastic known to have the lowest density of any commercial grade polymer available at 0.82 g/cc. Its typical color is a semi-opaque milky white, however in thinner gauges of sheet and film the material is transparent. TPX™ offers a unique combination of heat resistance and release characteristics. Because the surface tension of TPX™ is very low, the product displays excellent release and peeling characteristics. In addition, the extremely low density of TPX™ offers the potential for significant weight reduction of the final product. Applications include release films, lightweight structural parts, and hollow fibers. PMP is FDA compliant and used in many food and beverage applications.

Industry: Engineering; Semiconductor and ESD

Colors Available: Natural

Attributes: Chemical Resistance; Dielectric Properties; Transparent

Shapes: Extruded Slab; Compression Sheet; Extruded Rod; Extruded Film

Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

New suppliers have been added for this product during the past 60 days.  

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Water Absorption 0.010 %
@Time 86400 sec
0.010 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 25.0 MPa3630 psiASTM D638
Tensile Strength, Yield 29.6 MPa4300 psiASTM D882
Elongation at Break 19 %19 %ASTM D882
Tensile Modulus 1.90 GPa275 ksiASTM D882
Flexural Strength 40.0 MPa
@Strain 5.0 %
5800 psi
@Strain 5.0 %
ASTM D790
Flexural Modulus 1.50 GPa217 ksiASTM D790
Izod Impact, Notched 0.246 J/cm0.460 ft-lb/inASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10160 ohm-cm10160 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C261 °FASTM D648
 
Descriptive Properties
ColorTranslucent white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui TPX® MX004 Methylpentene Copolymer
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
Westlake Plastics PMP Film Made from TPX® Polymethylpentene Resin
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film
DuPont™ Kapton® 250FN029 Polyimide/FEP Composite Film

PWEST009 / 72713

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.