MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis Fibremod™ GE266WGU Polypropylene, 20% Chemically Coupled Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Fibremod" GE266WGU is a 20% chemically coupled glass fiber-reinforced polypropylene compound intended for injection molding. The product is available in natural color. This material shows excellent mechanical properties also at elevated temperatures.

Typical characteristics:

  • Long term high heat stabilized
  • UL Listed
  • Detergent resistant
Applications:
  • Tubs for washing machines
  • White goods
  • Washing machines, dishwashers and dryers
  • Appliances
To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183-1/Method A
Melt Flow 10.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 75.0 MPa
@Time 173000 sec
10900 psi
@Time 48.0 hour
ISO 527
Tensile Modulus 5.00 GPa
@Time 173000 sec
725 ksi
@Time 48.0 hour
ISO 527-2
Flexural Modulus 5.00 GPa
@Time 173000 sec
725 ksi
@Time 48.0 hour
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²ISO 180
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 - 80.0 °C104 - 176 °F
 220 - 260 °C428 - 500 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psi
 
Descriptive Properties
Flow front speed100 - 200 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9767 / 323124

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.