MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Poly Alloy Etoma™ ET4104 PC with Carbon Black
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Conductive

Material Notes: Etoma ET4104 resin is a conductive compound based on polycarbonate (PC) with carbon black The product made by ET4104 resin will have good heat resistance and stable surface resistivity

Information provided by Poly Alloy Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 64.7 MPa9390 psiASTM D638
Elongation at Break 18 %18 %ASTM D638
Flexural Strength 113 MPa16400 psiASTM D790
Flexural Modulus 3.33 GPa484 ksiASTM D790
Izod Impact, Notched 0.981 J/cm1.84 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1000 ohm - 1e+051000 ohm - 1e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 138 °C280 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 285 °C518 - 545 °F
Middle Barrel Temperature 275 - 295 °C527 - 563 °F
Front Barrel Temperature 290 - 300 °C554 - 572 °F
Nozzle Temperature 285 - 300 °C545 - 572 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 120 °C248 °F
Dry Time 4.00 - 8.00 hour4.00 - 8.00 hour
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPALLOY039 / 278318

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.