MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for 4000 Series Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 4000 Series Aluminum Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "4000 Series Aluminum Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.63 - 2.92 g/cc0.0950 - 0.105 lb/in³Average value: 2.70 g/cc Grade Count:49
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 39.0 - 18539.0 - 185Average value: 104 Grade Count:10
Hardness, Knoop 69.0 - 15069.0 - 150Average value: 124 Grade Count:5
Hardness, Rockwell A 46.8 - 47.046.8 - 47.0Average value: 46.9 Grade Count:3
Hardness, Rockwell B 74.0 - 75.074.0 - 75.0Average value: 74.6 Grade Count:5
Hardness, Vickers 30.0 - 13730.0 - 137Average value: 96.8 Grade Count:6
Tensile Strength, Ultimate 110 - 470 MPa16000 - 68200 psiAverage value: 294 MPa Grade Count:17
Tensile Strength, Yield 45.0 - 420 MPa6530 - 60900 psiAverage value: 244 MPa Grade Count:17
Elongation at Break 0.500 - 22.0 %0.500 - 22.0 %Average value: 6.21 % Grade Count:16
Modulus of Elasticity 77.0 - 90.0 GPa11200 - 13100 ksiAverage value: 82.6 GPa Grade Count:8
Poissons Ratio 0.3400.340Average value: 0.340 Grade Count:5
Machinability 70.0 %70.0 %Average value: 70.0 % Grade Count:3
Shear Strength 90.0 - 262 MPa13100 - 38000 psiAverage value: 175 MPa Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000382 - 0.00000499 ohm-cm0.00000382 - 0.00000499 ohm-cmAverage value: 0.00000440 ohm-cm Grade Count:10
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.7 - 23.7 µm/m-°C9.28 - 13.2 µin/in-°FAverage value: 20.2 µm/m-°C Grade Count:11
Specific Heat Capacity 0.850 J/g-°C0.203 BTU/lb-°FAverage value: 0.850 J/g-°C Grade Count:5
Thermal Conductivity 120 - 180 W/m-K833 - 1250 BTU-in/hr-ft²-°FAverage value: 146 W/m-K Grade Count:13
Melting Point 532 - 632 °C990 - 1170 °FAverage value: 586 °C Grade Count:9
Solidus 532 - 577 °C990 - 1070 °FAverage value: 565 °C Grade Count:9
Liquidus 571 - 632 °C1060 - 1170 °FAverage value: 607 °C Grade Count:9
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 349 - 413 °C660 - 775 °FAverage value: 367 °C Grade Count:7
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 70.7 - 98.7 %70.7 - 98.7 %Average value: 90.1 % Grade Count:50
Beryllium, Be 0.000300 - 0.0700 %0.000300 - 0.0700 %Average value: 0.00378 % Grade Count:18
Bismuth, Bi 0.0200 - 2.00 %0.0200 - 2.00 %Average value: 1.13 % Grade Count:5
Chromium, Cr 0.0100 - 0.250 %0.0100 - 0.250 %Average value: 0.107 % Grade Count:11
Copper, Cu 0.0300 - 5.00 %0.0300 - 5.00 %Average value: 0.739 % Grade Count:48
Iron, Fe 0.0900 - 5.40 %0.0900 - 5.40 %Average value: 0.815 % Grade Count:50
Magnesium, Mg 0.0100 - 2.00 %0.0100 - 2.00 %Average value: 0.455 % Grade Count:46
Manganese, Mn 0.0300 - 1.50 %0.0300 - 1.50 %Average value: 0.345 % Grade Count:40
Nickel, Ni 0.150 - 2.20 %0.150 - 2.20 %Average value: 1.05 % Grade Count:8
Silicon, Si 0.600 - 24.0 %0.600 - 24.0 %Average value: 7.40 % Grade Count:50
Titanium, Ti 0.00500 - 0.200 %0.00500 - 0.200 %Average value: 0.134 % Grade Count:25
Zinc, Zn 0.0500 - 10.7 %0.0500 - 10.7 %Average value: 0.385 % Grade Count:46

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for 6000 Series Aluminum Alloy
Overview of materials for 2000 Series Aluminum Alloy
Overview of materials for 3000 Series Aluminum Alloy
Overview of materials for 5000 Series Aluminum Alloy
Overview of materials for 7000 Series Aluminum Alloy

M01043 / 81685

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.