MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman DuraGrip™ DGR 6140 UT Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: DuraGrip® DGR 6140UT is an unfilled translucent Thermoplastic Elastomer (TPE). It is designed to process easily in injection molding and extrusion applications. DuraGrip® TPE features excellent soft touch feel, will bond to ABS, PC, Isoplast, clear copolyester and acrylics, and because it is translucent it is easily colored with a minimum of concentrate. DuraGrip® TPE is not hygroscopic and under normal conditions does not require drying.

Information provided by Advanced Polymer Alloys

Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/ccASTM D471; ISO 2781
Viscosity 302000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
302000 cP
@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3838Time of 5 seconds; ASTM D2240; ISO 48
Tensile Strength, Ultimate 8.929 MPa1295 psiASTM D412; ISO 37
Elongation at Break 644 %644 %ASTM D412; ISO 37
100% Modulus 1.20 MPa
@Strain 100 %
174 psi
@Strain 100 %
ASTM D412; ISO 37
 
Processing PropertiesMetricEnglishComments
Processing Temperature 216 °C420 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE)
A. Schulman DuraGrip™ 6150 BK Melt Processable Elastomer
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
ExxonMobil Santoprene® 8221-75M300 Thermoplastic Elastomer
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer

PAPA039 / 24106

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.