MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Overview of materials for Epoxy, Cast, Metal Filled
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Metal Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Master Bond is a leading manufacturer of high performance epoxy adhesives, sealants, coatings, potting/encapsulation compounds and impregnation resins. Our epoxies include one and two part formulations that can be cured at room temperature, with heat or exposure to UV light. Special formulations feature high electrical and/or thermal conductivity and wide service temperature ranges. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.959 - 3.12 g/cc0.0346 - 0.113 lb/in³Average value: 1.91 g/cc Grade Count:22
Water Absorption 0.0300 - 0.450 %0.0300 - 0.450 %Average value: 0.162 % Grade Count:5
Porosity 15.0 - 16.0 %15.0 - 16.0 %Average value: 15.7 % Grade Count:3
Viscosity 3000 - 160000 cP3000 - 160000 cPAverage value: 31000 cP Grade Count:11
Pore Size 12.7 - 15.2 microns0.500 - 0.600 milAverage value: 13.5 microns Grade Count:3
Linear Mold Shrinkage 0.000600 - 0.00400 cm/cm0.000600 - 0.00400 in/inAverage value: 0.00164 cm/cm Grade Count:9
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80.0 - 95.080.0 - 95.0Average value: 86.4 Grade Count:27
Tensile Strength, Ultimate 0.159 - 59.6 MPa23.0 - 8650 psiAverage value: 27.9 MPa Grade Count:24
Tensile Strength, Yield 6.89 - 20.7 MPa1000 - 3000 psiAverage value: 16.5 MPa Grade Count:5
Elongation at Break 0.000 - 130 %0.000 - 130 %Average value: 12.7 % Grade Count:11
Modulus of Elasticity 4.14 - 49.6 GPa600 - 7200 ksiAverage value: 12.9 GPa Grade Count:10
Flexural Yield Strength 3.45 - 56.0 MPa500 - 8130 psiAverage value: 34.4 MPa Grade Count:19
Flexural Modulus 9.00 - 10.8 GPa1310 - 1570 ksiAverage value: 9.67 GPa Grade Count:6
Compressive Yield Strength 41.4 - 108 MPa6000 - 15700 psiAverage value: 75.7 MPa Grade Count:23
Compressive Modulus 0.865 - 5.17 GPa126 - 750 ksiAverage value: 2.95 GPa Grade Count:9
Shear Strength 6.21 - 31.0 MPa900 - 4500 psiAverage value: 19.8 MPa Grade Count:17
 1.70 - 31.0 MPa
@Temperature -55.0 - 177 °C
247 - 4500 psi
@Temperature -67.0 - 351 °F
Average value: 14.0 MPa Grade Count:4
Adhesive Bond Strength 6.21 - 42.1 MPa900 - 6100 psiAverage value: 18.5 MPa Grade Count:7
 19.3053 - 27.9238 MPa
@Temperature -54.4 - 82.2 °C
2800.00 - 4050.01 psi
@Temperature -66.0 - 180 °F
Average value: 23.6 MPa Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 - 3.20e+16 ohm-cm1.00e+15 - 3.20e+16 ohm-cmAverage value: 1.04e+16 ohm-cm Grade Count:5
Dielectric Constant 4.50 - 21.44.50 - 21.4Average value: 7.15 Grade Count:6
Dielectric Strength 3.94 - 15.7 kV/mm100 - 400 kV/inAverage value: 13.1 kV/mm Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 - 53.0 µm/m-°C16.7 - 29.4 µin/in-°FAverage value: 40.4 µm/m-°C Grade Count:7
 30.06 - 125 µm/m-°C
@Temperature 25.0 - 125 °C
16.70 - 69.4 µin/in-°F
@Temperature 77.0 - 257 °F
Average value: 83.5 µm/m-°C Grade Count:8
Thermal Conductivity 0.724 - 1.20 W/m-K5.02 - 8.33 BTU-in/hr-ft²-°FAverage value: 1.05 W/m-K Grade Count:6
 19.0 - 20.5 W/m-K
@Temperature 100 - 100 °C
132 - 142 BTU-in/hr-ft²-°F
@Temperature 212 - 212 °F
Average value: 19.5 W/m-K Grade Count:3
Maximum Service Temperature, Air 57.0 - 210 °C135 - 410 °FAverage value: 125 °C Grade Count:15
Minimum Service Temperature, Air -60.0 - -20.0 °C-76.0 - -4.00 °FAverage value: -46.0 °C Grade Count:5
Glass Transition Temp, Tg 55.0 - 130 °C131 - 266 °FAverage value: 86.3 °C Grade Count:6
 
Processing PropertiesMetricEnglishComments
Processing Temperature 21.1 - 260 °C70.0 - 500 °FAverage value: 135 °C Grade Count:6
Cure Time 180 - 1440 min3.00 - 24.0 hourAverage value: 891 min Grade Count:7
 30.0 - 720 min
@Temperature 45.0 - 150 °C
0.500 - 12.0 hour
@Temperature 113 - 302 °F
Average value: 284 min Grade Count:11
Pot Life 30.0 - 100000 min30.0 - 100000 minAverage value: 4530 min Grade Count:23

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Solventless Epoxy Varnish, Electrical Insulation
Abatron Ferrobond-P™ Steel-Filled, Structural Adhesive Putty; Paste
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
Overview of materials for Epoxy Encapsulant, Unreinforced
Sulfur Hexafluoride, SF6

O1708 / 77893

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.