MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Aluminum 3004-H112
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 3000 Series Aluminum Alloy

Key Words: UNS A93004; AA3004-H112; Al3004-H112
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.72 g/cc0.0983 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 160 MPa
@Thickness 6.35 - 76.2 mm
>= 23200 psi
@Thickness 0.250 - 3.00 in
Tensile Strength, Yield >= 62.0 MPa
@Thickness 6.35 - 76.2 mm
>= 8990 psi
@Thickness 0.250 - 3.00 in
Elongation at Break 7.0 %
@Thickness 6.35 - 76.2 mm
7.0 %
@Thickness 0.250 - 3.00 in
Modulus of Elasticity 70.0 GPa10200 ksi
Poissons Ratio <= 0.35<= 0.35
Shear Modulus 25.0 GPa3630 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.5 µm/m-°C
@Temperature -50.0 - 20.0 °C
11.9 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.2 µm/m-°C
@Temperature 20.0 - 100 °C
12.9 µin/in-°F
@Temperature 68.0 - 212 °F
 24.1 µm/m-°C
@Temperature 20.0 - 200 °C
13.4 µin/in-°F
@Temperature 68.0 - 392 °F
 25.1 µm/m-°C
@Temperature 20.0 - 300 °C
13.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.893 J/g-°C0.213 BTU/lb-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 95.5 - 98.2 %95.5 - 98.2 %
Copper, Cu <= 0.25 %<= 0.25 %
Iron, Fe <= 0.70 %<= 0.70 %
Magnesium, Mg 0.80 - 1.3 %0.80 - 1.3 %
Manganese, Mn 1.0 - 1.5 %1.0 - 1.5 %
Other, each <= 0.050 %<= 0.050 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.30 %<= 0.30 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 3004-H19
Aluminum 3004-H32
Aluminum 3004-O
Aluminum 3004-H34
Aluminum 3004-H36

MA3004H112 / 109181

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.