MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Indium Corp. Indalloy® 7 In-Pb Solder Alloy
Categories: Metal; Nonferrous Metal; Indium Alloy; Lead Alloy; Solder/Braze Alloy

Material Notes: Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics of lead-indium as well as good thermal fatigue properties.

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 9.6
@Load 100 kg,
Time 30.0 sec
9.6
@Load 220 lb,
Time 0.00833 hour
Tensile Strength, Ultimate 32.2 MPa4670 psi
Elongation at Break 55 %55 %
Shear Strength 18.5 MPa2680 psiShear Bond Holding Strength
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000290 ohm-cm0.0000290 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 27.0 µm/m-°C
@Temperature 20.0 °C
15.0 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 22.0 W/m-K
@Temperature 85.0 °C
153 BTU-in/hr-ft²-°F
@Temperature 185 °F
Melting Point 184 - 210 °C363 - 410 °F
Solidus 184 °C363 °F
Liquidus 210 °C410 °F
 
Component Elements PropertiesMetricEnglishComments
Indium, In 50 %50 %
Lead, Pb 50 %50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cobalt Silicide, CoSi2
Chromium Silicide, CrSi2
Chromium Silicide, Cr3Si
Cerium Silicide, CeSi2
Barium Silicide, BaSi2

NNIN28 / 18484

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.