MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Angst+Pfister APSOplast® PBI High-performance plastic
Categories: Polymer; Thermoplastic; Polybenzimidazole (PBI)

Material Notes: It offers the highest temperature resistance and best retention of mechanical properties of all non-reinforced high-performance plastics. PBI is ionically very pure and does not degas (dry material). Thanks to its unique combination of properties, PBI can offer a solution where other plastics fail. This material is in high demand in the high-tech industry such as the semi-conductor, aeronautics, and astronautics industries. In these areas, PBI is primarily used for critical, complex components in order to reduce maintenance costs and win valuable operating time during production.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³DIN EN ISO 1183-1
Water Absorption  0.74 %
@Time 86400 sec
0.74 %
@Time 24.0 hour
DIN EN ISO 62
 1.37 %
@Time 346000 sec
1.37 %
@Time 96.0 hour
DIN EN ISO 62
Moisture Absorption 7.50 %7.50 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 375 MPa54400 psiDIN EN ISO 2039-1
Tensile Strength at Break 130 MPa18900 psi5 mm/min; DIN EN ISO 527
Tensile Strength 130 MPa18900 psiDIN EN ISO 527
Elongation at Break 3.0 %3.0 %5 mm/min; DIN EN ISO 527
Modulus of Elasticity 6.00 GPa870 ksiDIN EN ISO 527
Compressive Strength  58.0 MPa
@Strain 1 %,
Load 1.02 kg
8410 psi
@Strain 1 %,
Load 2.25 lb
5 mm/min; EN ISO 604
 118 MPa
@Strain 2 %,
Load 1.02 kg
17100 psi
@Strain 2 %,
Load 2.25 lb
5 mm/min; EN ISO 604
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²DIN EN ISO 179-1eU
Charpy Impact, Notched 0.250 J/cm²1.19 ft-lb/in²DIN EN ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmANSI/ESD STM 11.11
Dielectric Strength 28.0 kV/mm711 kV/inIEC 60243
Dielectric Loss Index 0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear  25.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
13.9 µin/in-°F
@Temperature 73.4 - 140 °F
 25.0 µm/m-°C
@Temperature 23.0 - 150 °C
13.9 µin/in-°F
@Temperature 73.4 - 302 °F
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 310 °C590 °Flong term
 500 °C932 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 425 °C797 °FDIN EN ISO 75 / A
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Glass Transition Temp, Tg 415 °C779 °FDIN 53765
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP074 / 250572

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.