MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Omnia Plastica Omniamid PA6 G - G - at 50% RH
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Cast nylon 6. The method of production of this polyamide (i.e. the polymerisation of the caprolactam directly in the mould) allows the production of stock shapes in larger than normal dimensions, such as big rings or very thick sheets. The general features are similar to those of PA66.6, which means that it is stiffer and more brittle than extruded PA6.

Features:

  • Wear resistance: good even in demanding environments. Tensile stress and compressive strength: the toughness is better than that of extruded PA6 and fatigue resistance is very high.
  • Self-lubricating: the friction coefficient is low and generally for sliding applications it does not require lubricators.
  • Ageing resistance: weatherproof, with good resistance at low temperature.
  • Natural colour.
Weak Point:

Like extruded nylon 6 it is hygroscopic. Due to its high fragility (in comparison with extruded PA6) it is advisable to use cast nylon for larger-sized pieces. Because of the molecular structure, large-sized cast pieces have a better quality than those of small dimensions.

Application:

  • Mechanical: thanks to the possibility of obtaining large-sized pieces this material is widely used in the mechanical field to produce large diameters gears, cams, pulleys, wheels and anti-wear guides. In the building of parts for construction machines, excavators and earthmovers it is used for gear wheels, guide bearings, sliding bearings, etc.
  • Food contact: generally it is not used in contact with food
  • Electrical: usage in the electrical field is to be avoided as the electrical properties change with the moisture content
  • Chemical: it is resistant to alkali, inorganic compounds and solvents.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO.1183 DIN.53479
Moisture Absorption at Equilibrium 2.4 %2.4 %50% relative humidity (beginning dry)
Water Absorption at Saturation 7.0 %7.0 %23°C (beginning dry)
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 100 MPa14500 psiISO2039.1 DIN.53456
Tensile Strength at Break 58.0 MPa8410 psiISO.527 DIN.53455
Elongation at Break 100 %100 %ISO.527 DIN.53455
Tensile Modulus 1.90 GPa276 ksiISO.527 DIN.53455
Compressive Strength 7.00 MPa1020 psi1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched NBNB7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 2.30 J/cm²10.9 ft-lb/in²ISO179/3C DIN.53453
Coefficient of Friction, Dynamic 0.420.42on dry ground steel; load =0.05MPa; speed =0.6 m/s (dry sample)
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 7.0
@Frequency 1e+6 Hz
7.0
@Frequency 1e+6 Hz
ISO.250 DIN.53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
dry sample
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°FDIN.52612 (dry sample)
Melting Point 220 °C428 °F
Maximum Service Temperature, Air 100 °C212 °FContinuous; 5000 hours based on a tensile stress of 50% at 23° C. (dry sample)
 160 °C320 °Fshort period, no load (dry sample)
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C205 °FISO.75 DIN.53461 (dry sample)
Minimum Service Temperature, Air -30.0 °C-22.0 °Fimpact conditions and heavy loads not considered (dry sample)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 15 000000 Copolyamide, 15% Glass Fiber
ASTM A36 Steel, bar
Overview of materials for Nylon 66/6
Mitsubishi Chemical Advanced Materials Nylatron™ 66 SA PA66 AE Polyamide 66, extruded

POMNIA07 / 55606

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.