MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Envalior ForTii® F12 PPA-GF40 FR(40) PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

ForTii® F12 has excellent balance of stiffness and toughness, suitable for high mechanical loaded application such as power connector or EV parts. F12 has high RTI electrical rating of 140°C at 0.75 mm and shows JEDEC Level 2 performance, enabling SMT process without deformation and low risk on blistering.

Features: Phosphorous free. 40% glass reinforced. Processing: Injection Molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³Dry; ISO 1183
Moisture Absorption 1.30 %1.30 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0085 cm/cm0.0085 in/inDry; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 170 MPa24700 psiDry; ISO 527-1/-2
 170 MPa24700 psiCond; ISO 527-1/-2
Elongation at Break 1.9 %1.9 %Dry; ISO 527-1/-2
 1.9 %1.9 %Cond; ISO 527-1/-2
Tensile Modulus 13.5 GPa1960 ksiDry; ISO 527-1/-2
 13.5 GPa1960 ksiCond; ISO 527-1/-2
Flexural Strength 260 MPa37700 psiCond; ISO 178
 280 MPa40600 psiDry; ISO 178
Flexural Modulus 14.5 GPa2100 ksiDry; ISO 178
 14.5 GPa2100 ksiCond; ISO 178
Charpy Impact Unnotched  6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
Cond; ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
Cond; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmDry; IEC 60093
 >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmCond; IEC 60093
Dielectric Constant  3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
Dry; IEC 60250
 3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
Cond; IEC 60250
 4.2
@Frequency 100 Hz
4.2
@Frequency 100 Hz
Dry; IEC 60250
 4.2
@Frequency 100 Hz
4.2
@Frequency 100 Hz
Cond; IEC 60250
Dielectric Strength 33.0 kV/mm838 kV/inDry; IEC 60243-1
 33.0 kV/mm838 kV/inCond; IEC 60243-1
Comparative Tracking Index 600 V600 VDry; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 µm/m-°C19.4 µin/in-°FASTM D696
CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FASTM D696
Melting Point 325 °C617 °F10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 305 °C581 °FDry; ISO 75-1/-2
UL RTI, Electrical 140 °C
@Thickness 0.350 mm
284 °F
@Thickness 0.0138 in
UL746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSM7904 / 291340

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.