MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Carbon Fiber/PTFE Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.17 - 1.54 g/cc0.0423 - 0.0556 lb/in³Average value: 1.32 g/cc Grade Count:75
Filler Content 5.00 - 50.0 %5.00 - 50.0 %Average value: 21.9 % Grade Count:29
Water Absorption 0.100 - 1.00 %0.100 - 1.00 %Average value: 0.572 % Grade Count:36
Moisture Absorption at Equilibrium 1.00 %1.00 %Average value: 1.00 % Grade Count:6
Additive Loading 20.0 - 30.0 %20.0 - 30.0 %Average value: 26.0 % Grade Count:5
Linear Mold Shrinkage 0.000200 - 0.0100 cm/cm0.000200 - 0.0100 in/inAverage value: 0.00260 cm/cm Grade Count:70
Linear Mold Shrinkage, Transverse 0.00200 - 0.0110 cm/cm0.00200 - 0.0110 in/inAverage value: 0.00730 cm/cm Grade Count:8
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110 - 120110 - 120Average value: 118 Grade Count:23
Tensile Strength, Ultimate 75.8 - 241 MPa11000 - 35000 psiAverage value: 177 MPa Grade Count:66
 105 - 170 MPa
@Temperature 60.0 - 150 °C
15200 - 24700 psi
@Temperature 140 - 302 °F
Average value: 135 MPa Grade Count:1
Tensile Strength, Yield 152 - 200 MPa22000 - 29000 psiAverage value: 186 MPa Grade Count:9
Elongation at Break 0.900 - 4.00 %0.900 - 4.00 %Average value: 2.59 % Grade Count:73
 2.50 - 3.80 %
@Temperature 60.0 - 150 °C
2.50 - 3.80 %
@Temperature 140 - 302 °F
Average value: 3.25 % Grade Count:1
Modulus of Elasticity 3.45 - 32.4 GPa500 - 4700 ksiAverage value: 16.0 GPa Grade Count:55
 8.30 - 22.5 GPa
@Temperature 60.0 - 150 °C
1200 - 3260 ksi
@Temperature 140 - 302 °F
Average value: 14.5 GPa Grade Count:1
Flexural Yield Strength 107 - 372 MPa15500 - 54000 psiAverage value: 266 MPa Grade Count:70
Flexural Modulus 2.76 - 24.8 GPa400 - 3600 ksiAverage value: 13.1 GPa Grade Count:72
Flexural Strain at Break 2.50 - 4.00 %2.50 - 4.00 %Average value: 3.30 % Grade Count:7
Compressive Yield Strength 89.6 - 172 MPa13000 - 25000 psiAverage value: 138 MPa Grade Count:11
Izod Impact, Notched 0.320 - 2.40 J/cm0.600 - 4.50 ft-lb/inAverage value: 0.891 J/cm Grade Count:62
Izod Impact, Unnotched 4.00 - 10.7 J/cm7.50 - 20.0 ft-lb/inAverage value: 7.01 J/cm Grade Count:42
Charpy Impact Unnotched 2.50 - 6.80 J/cm²11.9 - 32.4 ft-lb/in²Average value: 4.32 J/cm² Grade Count:13
 2.80 - 4.00 J/cm²
@Temperature -40.0 - -20.0 °C
13.3 - 19.0 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 3.33 J/cm² Grade Count:7
Charpy Impact, Notched 0.400 - 1.10 J/cm²1.90 - 5.24 ft-lb/in²Average value: 0.873 J/cm² Grade Count:11
 0.300 - 0.800 J/cm²
@Temperature -40.0 - -20.0 °C
1.43 - 3.81 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.629 J/cm² Grade Count:7
Coefficient of Friction 0.100 - 0.6000.100 - 0.600Average value: 0.239 Grade Count:8
Coefficient of Friction, Static 0.0900 - 0.5600.0900 - 0.560Average value: 0.231 Grade Count:8
K (wear) Factor 10.1 - 30.2 x 10-8 mm³/N-M5.00 - 15.0 x 10-10 in³-min/ft-lb-hrAverage value: 16.3 x 10-8 mm³/N-M Grade Count:10
Limiting Pressure Velocity 0.771 - 3.30 MPa-m/sec22000 - 94200 psi-ft/minAverage value: 1.45 MPa-m/sec Grade Count:5
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00 - 1.00e+8 ohm-cm1.00 - 1.00e+8 ohm-cmAverage value: 811 ohm-cm Grade Count:50
Surface Resistance 1.00 - 1.00e+6 ohm1.00 - 1.00e+6 ohmAverage value: 30000 ohm Grade Count:20
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 - 39.6 µm/m-°C7.78 - 22.0 µin/in-°FAverage value: 21.9 µm/m-°C Grade Count:22
 22.0 - 22.0 µm/m-°C
@Temperature 70.0 - 120 °C
12.2 - 12.2 µin/in-°F
@Temperature 158 - 248 °F
Average value: 22.0 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 142 - 142 µm/m-°C
@Temperature 70.0 - 120 °C
78.9 - 78.9 µin/in-°F
@Temperature 158 - 248 °F
Average value: 142 µm/m-°C Grade Count:1
Thermal Conductivity 0.300 - 1.15 W/m-K2.08 - 8.00 BTU-in/hr-ft²-°FAverage value: 0.571 W/m-K Grade Count:14
Melting Point 249 - 275 °C480 - 527 °FAverage value: 261 °C Grade Count:10
Maximum Service Temperature, Air 100 - 170 °C212 - 338 °FAverage value: 137 °C Grade Count:7
Deflection Temperature at 0.46 MPa (66 psi) 232 - 270 °C450 - 518 °FAverage value: 256 °C Grade Count:31
Deflection Temperature at 1.8 MPa (264 psi) 227 - 260 °C440 - 500 °FAverage value: 248 °C Grade Count:69
Vicat Softening Point 200 - 255 °C392 - 491 °FAverage value: 241 °C Grade Count:10
Flammability, UL94 HBHBGrade Count:35
 
Processing PropertiesMetricEnglishComments
Processing Temperature 274 - 300 °C525 - 572 °FAverage value: 285 °C Grade Count:22
Nozzle Temperature 280 - 300 °C536 - 572 °FAverage value: 290 °C Grade Count:7
Melt Temperature 260 - 310 °C500 - 590 °FAverage value: 292 °C Grade Count:39
Mold Temperature 65.6 - 121 °C150 - 250 °FAverage value: 91.5 °C Grade Count:56
Drying Temperature 75.0 - 107 °C167 - 225 °FAverage value: 85.2 °C Grade Count:37
Moisture Content 0.100 - 0.200 %0.100 - 0.200 %Average value: 0.177 % Grade Count:26
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:17
Injection Pressure 68.9 - 124 MPa10000 - 18000 psiAverage value: 101 MPa Grade Count:34

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
3M S38HS Glass Bubbles
3M S38 Glass Bubbles
3M S35 Glass Bubbles

O2528 / 78026

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.