MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Rotational Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.932 - 0.947 g/cc0.0337 - 0.0342 lb/in³Average value: 0.937 g/cc Grade Count:41
Environmental Stress Crack Resistance 4.00 - 1000 hour4.00 - 1000 hourAverage value: 477 hour Grade Count:30
 19.0 - 28.0 hour
@Temperature 50.0 - 50.0 °C
19.0 - 28.0 hour
@Temperature 122 - 122 °F
Average value: 693 hour Grade Count:7
Melt Flow 1.70 - 7.00 g/10 min1.70 - 7.00 g/10 minAverage value: 4.70 g/10 min Grade Count:40
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55.0 - 65.055.0 - 65.0Average value: 58.2 Grade Count:9
Tensile Strength, Ultimate 11.7 - 39.0 MPa1700 - 5660 psiAverage value: 24.2 MPa Grade Count:9
Tensile Strength, Yield 14.0 - 24.1 MPa2030 - 3500 psiAverage value: 19.0 MPa Grade Count:39
Elongation at Break 340 - 1500 %340 - 1500 %Average value: 965 % Grade Count:19
Elongation at Yield 8.00 - 17.4 %8.00 - 17.4 %Average value: 12.5 % Grade Count:13
Flexural Modulus 0.428 - 0.896 GPa62.1 - 130 ksiAverage value: 0.643 GPa Grade Count:40
Izod Impact, Notched 0.530 - 5.30 J/cm0.993 - 9.93 ft-lb/inAverage value: 2.12 J/cm Grade Count:5
Charpy Impact, Notched 1.80 - 15.0 J/cm²8.57 - 71.4 ft-lb/in²Average value: 6.27 J/cm² Grade Count:3
 >= 15.0 J/cm²
@Temperature -30.0 - -30.0 °C
>= 71.4 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 15.0 J/cm² Grade Count:1
Tensile Impact Strength 145 - 163 kJ/m²69.0 - 77.6 ft-lb/in²Average value: 154 kJ/m² Grade Count:4
Dart Drop Total Energy 190 - 210 J/cm0.356 - 0.393 ft-lb/milAverage value: 206 J/cm Grade Count:14
Dart Drop 142 - 152 g/micron3610 - 3860 g/milAverage value: 151 g/micron Grade Count:13
 
Thermal PropertiesMetricEnglishComments
Melting Point 122 - 129 °C252 - 264 °FAverage value: 126 °C Grade Count:14
Crystallization Temperature 112 - 114 °C234 - 237 °FAverage value: 113 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 47.0 - 76.0 °C117 - 169 °FAverage value: 62.2 °C Grade Count:26
Deflection Temperature at 1.8 MPa (264 psi) 37.3 - 42.0 °C99.1 - 108 °FAverage value: 39.5 °C Grade Count:8
Vicat Softening Point 108 - 122 °C226 - 252 °FAverage value: 116 °C Grade Count:16
Brittleness Temperature -100 - -70.0 °C-148 - -94.0 °FAverage value: -72.1 °C Grade Count:14
 
Processing PropertiesMetricEnglishComments
Melt Temperature 131 - 315 °C268 - 599 °FAverage value: 208 °C Grade Count:13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Medium Density Polyethylene (MDPE), Molded
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight

O3906 / 78270

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.