MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Conventus Polymers DURAFILL PPH GF20 Polypropylene, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: DURAFILL PPH GF20 is a polypropylene filled with 20% glass fiber for injection molding.

Information provided by Conventus Polymers LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Yield 75.0 MPa10900 psiASTM D638
Elongation at Break 6.0 %6.0 %ASTM D638
Tensile Modulus 4.80 GPa696 ksiASTM D638
Flexural Modulus 4.50 GPa653 ksiASTM D790
Izod Impact, Notched 1.10 J/cm2.06 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 150 °C302 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 190 - 220 °C374 - 428 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature  80.0 °C
@Time 3600 sec
176 °F
@Time 1.00 hour
Dehumidify
 80.0 °C
@Time 7200 sec
176 °F
@Time 2.00 hour
Hot-air
Injection Pressure 80.0 - 100 MPa11600 - 14500 psi
Screw Speed 50 - 200 rpm50 - 200 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCONV771 / 265851

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.