MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

BASF 3D Ultrafuse® PPSU Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Components: BASF Polyphenylsulfone (PPSU) based filament for Fused Filament Fabrication.

Product Description: Outstanding thermal stability, good chemical resistance and high strength are the key features of Ultrafuse® PPSU. Parts produced by fused filament fabrication show often mechanical limitations in z-direction - the good layer adhesion of Ultrafuse® PPSU leads to balanced flexural strength properties between z- and x-direction. Ultrafuse® PPSU can be used for functional applications which require a high mechanical strength as well as a high heat distortion temperature – properties, where existing 3D printing materials often show limitations.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.272 g/cc0.04595 lb/in³Printed Part; ISO 1183-1
Melt Flow 20.8608 g/10 min
@Load 5.00 kg,
Temperature 360 °C
20.8608 g/10 min
@Load 11.0 lb,
Temperature 680 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 49.0 MPa7110 psiZX: Upright; ISO 527
 74.5 MPa10800 psiXY: Flat; ISO 527
Elongation at Break 2.9 %2.9 %ZX: Upright; ISO 527
 7.3 %7.3 %XY: Flat; ISO 527
Modulus of Elasticity 2.15 GPa312 ksiYoung's, ZX: Upright; ISO 527
 2.221 GPa322.1 ksiYoung's, XY: Flat; ISO 527
Flexural Strength 88.9 MPa12900 psiZX: Upright; ISO 178
 105 MPa15200 psiXY: Flat; ISO 178
 114 MPa16500 psiXZ: On its edge; ISO 178
Flexural Modulus 1.70 GPa247 ksiZX: Upright; ISO 178
 1.91 GPa277 ksiXZ: On its edge; ISO 178
 1.94 GPa281 ksiXY: Flat; ISO 178
Flexural Strain at Break 6.8 %6.8 %ZX: Upright; ISO 178
Izod Impact, Notched (ISO) 5.30 kJ/m²2.52 ft-lb/in²ZX: Upright; ISO 180
 13.7 kJ/m²6.52 ft-lb/in²XY: Flat; ISO 180
 15.8 kJ/m²7.52 ft-lb/in²XZ: On its edge; ISO 180
Izod Impact, Unnotched (ISO) 21.0 kJ/m²9.99 ft-lb/in²ZX: Upright; ISO 180
 NBNBXY: Flat; ISO 180
 NBNBXZ: On its edge; ISO 180
Charpy Impact Unnotched 1.63 J/cm²7.76 ft-lb/in²ZX: Upright; ISO 179-2
 22.48 J/cm²107.0 ft-lb/in²XY: Flat; ISO 179-2
 27.05 J/cm²128.7 ft-lb/in²XZ: On its edge; ISO 179-2
Charpy Impact, Notched 0.570 J/cm²2.71 ft-lb/in²ZX: Upright; ISO 179-2
 1.50 J/cm²7.14 ft-lb/in²XZ: On its edge; ISO 179-2
 2.18 J/cm²10.4 ft-lb/in²XY: Flat; ISO 179-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.60e+15 ohm-cm5.60e+15 ohm-cmXY: Flat; IEC 62631-3-1
Surface Resistance 4.10e+15 ohm4.10e+15 ohmXY: Flat; IEC 62631-3-2
Dielectric Strength 18.5 kV/mm470 kV/inXY: Flat, orthogonal; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C30.6 µin/in-°FISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 211 °C412 °FISO 75-2
Vicat Softening Point 217 °C
@Load 5.10 kg
423 °F
@Load 11.2 lb
ISO 306
Glass Transition Temp, Tg 222 °C432 °FISO 11357-2
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Glow Wire Test  960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-11
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-11
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 - 220 °C392 - 428 °FBed, Bed Material: Glass
Nozzle Temperature 390 - 410 °C734 - 770 °F
Drying Temperature 125 °C257 °FSpools can be dried in a vacuum dryer
Dry Time 8.00 hour8.00 hour
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Build Chamber Temperature170 – 210°C
Nozzle Diameter=0.4 mm
Print speed25-100 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF3D015 / 312256

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.