MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Imerys DB-Float™ Kaolin
Categories: Ceramic; Clay; Kaolin Clay; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes:

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.60 g/cc2.60 g/cc
Brightness 80 %80 %G.E. Brightness
Particle Size 0.50 µm0.50 µm27% finer than
 1.0 µm1.0 µm46.5% finer than
 2.0 µm2.0 µm60% finer than
 5.0 µm5.0 µm81.5% finer than
 10 µm10 µm93.5% finer than
 20 µm20 µm99% finer than
Particle Mesh Size 325 Mesh325 Mesh0.5% retained
pH 4.5 - 6.54.5 - 6.5
 
Component Elements PropertiesMetricEnglishComments
Al2O3 39.2 %39.2 %
CaO 0.040 %0.040 %
Fe2O3 0.50 %0.50 %
K2O 0.13 %0.13 %
Loss on Ignition(%) 13.6 %13.6 %
MgO 0.040 %0.040 %
Na2O 0.090 %0.090 %
SiO2 45.5 %45.5 %
TiO2 1.66 %1.66 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Imerys G-20 HP Feldspar
Illite KAl2(AlSi3O10)-(OH)2
CIMBAR Suspengel™ 325 Plus High Purity Bentonite, Industrial Grade
CIMBAR Suspengel™ 30 High Purity Bentonite, Industrial Grade
CIMBAR Suspengel™ 16 High Purity Bentonite, Industrial Grade

CIMERY035 / 88385

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.