MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Red Brass, UNS C23000 (230 Brass), M20 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: As Hot Rolled

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Spot Weld

Common Fabrication Processes: Blanking; Coining; Drawing; Etching; Forming and Bending; Heading and Upsetting; Piercing and Punching; Roll Threading and Knurling; Shearing; Spinning; Squeezing and Swaging; Stamping

Typical uses: Etching Parts; Trim; Weather Strip; Kick Plates; Badges; Coinage; Compacts; Costume Jewelry; Dials; Fire Extinguisher Cases; Lipstick Containers; Medallions; Nameplates; Plaques; Rouge Boxes; Tokens; Zippers; Conduit; Rotor Bars, AC Motors; Screw Shells; Sockets; Eyelets; Fasteners; Condenser Tubes; Fire Extinguishers; Flexible Metal Hose; Heat Exchanger Shells; Heat Exchangers; Pickling Crates; Pump Cylinder Liners; Radiator Cores; Tags; Tubing for Heat Exchangers; Tubing for Instrumentation; Fire Hose Couplings; Fittings; J-Bends; Pipe; Pipe Nipples; Pipe Service Lines; Pump Lines; Service Lines; Traps

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 290 MPa42000 psi
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 44.1 GPa6400 ksi
Poissons Ratio 0.330.33Calculated
Machinability 30 %30 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000460 ohm-cm0.00000460 ohm-cm37% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.7 µm/m-°C
@Temperature 20.0 - 300 °C
10.4 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 13.3 W/m-K92.0 BTU-in/hr-ft²-°F
Melting Point 988 - 1030 °C1810 - 1880 °F
Solidus 988 °C1810 °F
Liquidus 1030 °C1880 °F
Annealing Point 427 - 732 °C800 - 1350 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 788 - 899 °C1450 - 1650 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 84 - 86 %84 - 86 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.050 %<= 0.050 %
Zinc, Zn 13.9 - 16 %13.9 - 16 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC23000x1 / 292895

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.