MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Air-Hardening Steel
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Air-Hardening Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.39 - 8.03 g/cc0.267 - 0.290 lb/in³Average value: 7.76 g/cc Grade Count:52
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 192 - 594192 - 594Average value: 354 Grade Count:16
Hardness, Knoop 431 - 724431 - 724Average value: 604 Grade Count:8
Hardness, Rockwell C 10.0 - 66.510.0 - 66.5Average value: 56.8 Grade Count:44
Hardness, Vickers 200 - 703200 - 703Average value: 513 Grade Count:10
Tensile Strength, Ultimate 610 - 2380 MPa88500 - 345000 psiAverage value: 1780 MPa Grade Count:15
Tensile Strength, Yield 470 - 2100 MPa68200 - 305000 psiAverage value: 1460 MPa Grade Count:15
Elongation at Break 1.00 - 15.0 %1.00 - 15.0 %Average value: 8.91 % Grade Count:15
Reduction of Area 2.00 - 65.0 %2.00 - 65.0 %Average value: 32.4 % Grade Count:10
Modulus of Elasticity 138 - 221 GPa20000 - 32100 ksiAverage value: 202 GPa Grade Count:29
Bulk Modulus 160 GPa23200 ksiAverage value: 160 GPa Grade Count:10
Poissons Ratio 0.3000.300Average value: 0.300 Grade Count:3
Machinability 30.0 - 80.0 %30.0 - 80.0 %Average value: 60.9 % Grade Count:25
Shear Modulus 77.0 - 80.0 GPa11200 - 11600 ksiAverage value: 79.3 GPa Grade Count:10
Izod Impact Unnotched 10.8 - 229 J8.00 - 169 ft-lbAverage value: 66.8 J Grade Count:6
Charpy Impact 6.10 - 205 J4.50 - 151 ft-lbAverage value: 45.6 J Grade Count:15
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.45 - 14.7 µm/m-°C4.14 - 8.17 µin/in-°FAverage value: 12.3 µm/m-°C Grade Count:29
Thermal Conductivity 20.4 - 32.9 W/m-K142 - 228 BTU-in/hr-ft²-°FAverage value: 26.2 W/m-K Grade Count:7
Transformation Temperature 785 - 857 °C1450 - 1570 °FAverage value: 843 °C Grade Count:5
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 1550 °C302 - 2830 °FAverage value: 735 °C Grade Count:18
Annealing Temperature 730 - 900 °C1350 - 1650 °FAverage value: 831 °C Grade Count:10
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.00 - 7.00 %2.00 - 7.00 %Average value: 4.00 % Grade Count:3
Carbon, C 0.230 - 2.85 %0.230 - 2.85 %Average value: 1.00 % Grade Count:54
Chromium, Cr 0.400 - 27.0 %0.400 - 27.0 %Average value: 6.83 % Grade Count:56
Cobalt, Co 2.80 - 30.0 %2.80 - 30.0 %Average value: 15.9 % Grade Count:6
Copper, Cu 0.250 %0.250 %Average value: 0.250 % Grade Count:4
Iron, Fe 19.0 - 98.6 %19.0 - 98.6 %Average value: 85.3 % Grade Count:59
Manganese, Mn 0.250 - 3.00 %0.250 - 3.00 %Average value: 0.796 % Grade Count:46
Molybdenum, Mo 0.330 - 5.50 %0.330 - 5.50 %Average value: 1.45 % Grade Count:55
Nickel, Ni 0.250 - 22.0 %0.250 - 22.0 %Average value: 5.13 % Grade Count:13
Phosphorus, P 0.00150 - 0.300 %0.00150 - 0.300 %Average value: 0.0442 % Grade Count:17
Silicon, Si 0.100 - 1.25 %0.100 - 1.25 %Average value: 0.707 % Grade Count:45
Sulfur, S 0.00300 - 0.0900 %0.00300 - 0.0900 %Average value: 0.0249 % Grade Count:21
Titanium, Ti 0.500 - 4.00 %0.500 - 4.00 %Average value: 2.13 % Grade Count:3
Tungsten, W 0.500 - 8.50 %0.500 - 8.50 %Average value: 2.20 % Grade Count:12
Vanadium, V 0.130 - 10.3 %0.130 - 10.3 %Average value: 2.09 % Grade Count:35

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Cold Work Steel
Overview of materials for Hot Work Steel
Overview of materials for Oil-Hardening Steel
Overview of materials for Mold Steel
Overview of materials for Water-Hardening Steel

M01031 / 81704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.