MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite XB-22 Phenolic Nocolac Molding Compound
Categories: Polymer; Thermoset; Phenolic; Phenolic/Glass Fiber SMC

Material Notes: XB-22 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is formulated for low thermal conductivity.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/ccASTM D792
Apparent Bulk Density 0.700 g/cc0.0253 lb/in³Powder; ASTM D1895
Water Absorption 0.11 %
@Time 86400 sec
0.11 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0025 cm/cm0.0025 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8383ASTM D785
Tensile Strength 86.0 MPa12500 psiASTM D638
Flexural Strength 140 MPa20300 psiASTM D790
Flexural Modulus 10.3 GPa1490 ksiASTM D790
Compressive Strength 210 MPa30500 psiASTM D695
Izod Impact, Notched 0.400 J/cm0.749 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  11.5 kV/mm
@Frequency 60 Hz
292 kV/in
@Frequency 60 Hz
SS, dry; ASTM D149
 15.0 kV/mm
@Frequency 60 Hz
381 kV/in
@Frequency 60 Hz
ST, dry; ASTM D149
Arc Resistance 50 sec50 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 13.0 µm/m-°C7.22 µin/in-°FASTM E831
Thermal Conductivity 0.360 W/m-K2.50 BTU-in/hr-ft²-°FASTM C518
Maximum Service Temperature, Air 150 °C302 °FUL 746B Temperature Index
Deflection Temperature at 1.8 MPa (264 psi) 170 °C338 °FAs Molded; ASTM D648A
 >= 282 °C>= 540 °FPost Baked; ASTM D648A
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 V-1
@Thickness 3.20 mm
V-1
@Thickness 0.126 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite FM 4005X4649 Phenolic Molding Compound
Sumitomo Bakelite FM 4005X4648 Phenolic Novolac Molding Compound
Bakelite® PF 1110 Phenolic Molding Compound

PSUMIT209 / 194014

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.